MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Henkel Hysol EA 9321 Paste Adhesive System
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Thixotropic adhesive that yields tough, durable bonds over a wide temperature range.
    Applications:
  • Potting
  • Structural Repair

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Storage Temperature 4.00 °C39.2 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 49.0 MPa7110 psi
Elongation at Break 6.0 %6.0 %
Tensile Modulus 2.90 GPa421 ksi
Compressive Strength 62.1 MPa9010 psi
Compressive Modulus 1.96 GPa284 ksi
Adhesive Bond Strength  11.7 MPa
@Temperature 93.0 °C
1700 psi
@Temperature 199 °F
Tensile Lap Shear
 20.7 MPa
@Temperature -55.0 °C
3000 psi
@Temperature -67.0 °F
Tensile Lap Shear
 27.6 MPa
@Temperature 25.0 °C
4000 psi
@Temperature 77.0 °F
Tensile Lap Shear
Peel Strength 1.00 kN/m5.71 pliBell Peel
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 min
@Temperature 82.0 °C
1.00 hour
@Temperature 180 °F
 7200 - 10100 min
@Temperature 25.0 °C
120 - 168 hour
@Temperature 77.0 °F
Pot Life 40 min40 min
 
Descriptive Properties
ConsistencyThixotropic
Form2 parts
Mix Ratio, Part A:Part B100:50
Peel StrengthLow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Henkel Hysol EA 9313 Paste Adhesive System
Henkel Hysol EA 9320NA Paste Adhesive System
Henkel Hysol EA 9330.3 Paste Adhesive System
Henkel Hysol EA 9330 Paste Adhesive System
Henkel Hysol EA 9323 Paste Adhesive System

PHENK807 / 146812

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.