MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chevron Phillips HiD® 94312 HDPE Extrusion Coating Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: Resin Type: Melt blend, FDA approved

Characteristics:

  • Good processability
  • Good drawdown capability
  • Improved MVTR properties
  • Grease resistance

Applications:

  • MVTR applications
  • Release liners
  • Cup stock

Information provided by Chevron Phillips.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.590 g/cc0.0213 lb/in³ASTM D1895
Density 0.943 g/cc0.0341 lb/in³ASTM D1505
Melt Flow 12 g/10 min12 g/10 minCondition 190/2.16; ASTM D1238
Neck In 8.60 cm3.39 inAt 900 fpm
 9.50 cm3.74 inAt 700 fpm
 10.2 cm4.02 inAt 500 fpm
 11.1 cm4.37 inAt 300 fpm
 
Mechanical PropertiesMetricEnglishComments
Coefficient of Friction 0.280.28Poly to poly surface tested
Coefficient of Friction, Static 0.320.32Poly to poly surface tested
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 108 °C226 °FASTM D1525
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
MVTR, 100°F14.9 gms/24hrs/m2at 100°F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NOVA Chemicals Sclair® 35BE HDPE Extrusion Resin
NOVA Chemicals Sclair® 94D1 HDPE Extrusion Resin
JPJ Technologies 1600J HDPE Extrusion
Chevron Phillips Marlex® K608 HDPE Extrusion Molding Resin
Braskem GP5550BK HDPE High Density Extrusion Polyethylene

PCHEVD014 / 20633

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.