MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

HM 35 Carbon fiber used in carbon prosthesis
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Key Words: medical, surgical
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.79 g/cc0.0647 lb/in³
Filament Diameter 6.7 µm6.7 µm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 2350 MPa341000 psi
Elongation at Break 0.60 %0.60 %
Modulus of Elasticity 358 GPa51900 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear -0.500 µm/m-°C
@Temperature 100 °C
-0.278 µin/in-°F
@Temperature 212 °F

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Toho Tenax Besfight® MC Type I (3000 Filament) Nickel Coated Carbon Fiber
Hexcel® HexTow® AS4 3K Standard Modulus Carbon Fiber (3000 Filaments)
Hexcel® HexTow® PV42/850 Carbon Fiber
Solvay Thornel® P-25 2K Carbon Fiber, Pitch Precursor
Solvay THORNEL® P-25 Pitch-Based Fiber

PMEDIC04 / 52564

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.