MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Techical Ceramics Ekatherm® Silicon Nitride
Categories: Ceramic; Carbide

Material Notes:

Information provided by 3M Technical Ceramics, formerly ESK Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density >= 3.24 g/cc>= 0.117 lb/in³DIN EN 623-2
Porosity <= 0.50 %<= 0.50 %DIN EN 623-2
Grain Size <= 2.0 µm<= 2.0 µm
Weibull Modulus 1515[m]; DIN EN 843-5
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 15
@Pressure 100 MPa
15
@Pressure 14500 psi
DIN EN 843-4
Hardness, Vickers 15
@Pressure 1000 MPa
15
@Pressure 145000 psi
DIN EN 843-4
Tensile Modulus 300 GPa43500 ksiYoung's; DIN EN 843-2
Flexural Strength 700 MPa102000 psi4-pt bending; DIN EN 843-1
Compressive Strength >= 2500 MPa>= 363000 psiDIN 51104
Poissons Ratio 0.280.28DIN EN 843-2
Fracture Toughness 7.00 MPa-m½6.37 ksi-in½SENB
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+11 ohm-cm>= 1.00e+11 ohm-cmDIN EN 50359
 
Thermal PropertiesMetricEnglishComments
CTE, linear  2.50 µm/m-°C
@Temperature 25.0 - 500 °C
1.39 µin/in-°F
@Temperature 77.0 - 932 °F
DIN EN 821-1
 3.90 µm/m-°C
@Temperature 500 - 1000 °C
2.17 µin/in-°F
@Temperature 932 - 1830 °F
DIN EN 821-1
Specific Heat Capacity 0.650 J/g-°C0.155 BTU/lb-°FC DIN EN 821-3
Thermal Conductivity 27.0 W/m-K187 BTU-in/hr-ft²-°FDIN EN 821-2
 
Descriptive Properties
Thermal Stress27 W/mmR2= R1-λ
 672 KR1 = sB·(1-ν)/(α·E)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Techical Ceramics Ekasic® S Silicon Nitride
CeramTec SL 200 BG Silicon Nitride, Si3N4-Y2O3
Silicon Nitride
Ceradyne Ceralloy® 147-5 Silicon Nitride
Goodfellow High Thermal Conductivity Silicon Nitride

CESK13 / 183305

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.