Braskem 6D43 Polypropylene Random Copolymer
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
Material Notes:
Description: Consistent processability, good spinning characteristics
Applications: Suggested uses include fiber spinning processes
Information provided by Braskem
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Melt Flow
35
g/10 min
@Load 2.16 kg,
Temperature 230 °C
35
g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell R
80
80
ASTM D785
Tensile Strength, Yield
24.0
MPa
3480
psi
50 mm/min; ASTM D638
Elongation at Yield
10 %
10 %
50 mm/min; ASTM D638
Flexural Modulus, 1% Secant
827
MPa
120000
psi
1.3 mm/min; ASTM D790A
Izod Impact, Notched
0.430
J/cm
0.806
ft-lb/in
ASTM D256A
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
BP Amoco 8410 Polypropylene Random Copolymer
Braskem 6D83K Polypropylene Random Copolymer
Braskem 6D83G Polypropylene Random Copolymer
Braskem RP350 Polypropylene Random Copolymer
A. Schulman PP 1632-01 Polypropylene Random Copolymer
PBRASK2060 / 199941
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.