MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hogen H20S, 26 Silver/74 Tungsten PM Metal Composite
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Precious Metal; Silver Alloy; Refractory Metal; Tungsten Alloy

Material Notes: RWMA Class EDM

DURAKUT Copper-Tungsten and Silver-Tungsten are manufactured as electrode materials for EDM (Electrical Discharge Machining), ECM (Electro Chemical Machining) and ECD (Electro Chemical Deburring).

Hogan DURAKUT materials are also manufactured by the powder metallurgy techniques of pressing, sintering and infiltrating tungsten with copper or silver. DURAKUT is produced under the same rigid manufacturing procedures and strict quality control supervision as Duralloy. This assures a high performance electrode providing greater cutting stability, excellent machinability and reduced down time. For extremely close tolerance work, Durakut holds dimensions and will not break down due to porosity and other structural deficiencies sometimes found in other Copper-Tungsten electrode alloys.

DURAKUT Copper-Tungsten is well suited for machining carbide dies. Further more, it offers greater cutting stability in machining refractory metals and exotics.

Tungsten alloys used for EDM and ECM applications are far superior when fine surface finishes, deep narrow slots or ribs and small precise holes are required. Tungsten alloys are preferred when matching extremely detailed sections. In the ECM process, Copper-Tungsten withstands erosive effects of short circuit malfunctions far better than other materials.

Data provided by Hogen Industries.

Key Words: Hogen Industries Powder Metallurgy Metal Composite; Tungsten Alloys, Silver Alloys
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density >= 15.1 g/cc>= 0.546 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 8787
Tensile Strength, Ultimate 483 MPa70100 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000340 ohm-cm0.00000340 ohm-cm
 
Component Elements PropertiesMetricEnglishComments
Silver, Ag 26 %26 %
Tungsten, W 74 %74 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hogen H50S, 50 Silver/50 Tungsten PM Metal Composite
Epoxy Technology EPO-TEK® H20S Electrically Conductive, Silver Epoxy for Die Stamping
CMW® ELKONIUM 46 Silver Alloy
Hogen Duralloy H1W 55 Tungsten/45 Copper PM Metal Composite
Hogen Duralloy H3W 68 Tungsten/32 Copper PM Metal Composite

NHOG02 / 17310

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.