MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Astryn BA45H Polypropylene Copolymer, Flame Retardant  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes:
Key Features: medium melt flow, medium modulus, flame retardant polypropylene copolymer, UL 94 V-2 flames, good electrical properties and insulating characteristics, good aesthetics and colorability, good processability

Applications: battery cases and chargers, furniture, small appliances

Description: Astryn BA45H conventional melt flow, UL 94 V-2 flame tretardant polypropylene copolymer has an excellent cobination of properties and processability. It was designed for application which require flame and heat resistance, along with good electrical properties, high impact strenght and good surface quality.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³ASTM D792B
Linear Mold Shrinkage 0.016 cm/cm0.016 in/inTool, Montell
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
10 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8484ASTM D785
Tensile Strength, Yield 23.0 MPa3340 psiASTM D638
Elongation at Break 100 %100 %ASTM D638
Flexural Modulus, 1% Secant 1100 MPa160000 psi0.05 in/min; ASTM D790A
Izod Impact, Notched 1.10 J/cm2.06 ft-lb/inASTM D256A
Gardner Impact 28.0 J20.7 ft-lbASTM D3029
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 8.90e+16 ohm-cm8.90e+16 ohm-cmASTM D257
Dielectric Strength 27.1 kV/mm688 kV/inASTM D149
Arc Resistance 133 sec133 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °FASTM D648
UL RTI, Mechanical with Impact 115 °C
@Thickness 3.00 mm
239 °F
@Thickness 0.118 in
ASTM UL94
Flammability, UL94 V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
Oxygen Index 28 %28 %ASTM D2863

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Moplen HP550J Polypropylene Homopolymer
LyondellBasell Astryn BA905-74 Polypropylene Copolymer, Flame Retardant
Aurora Plastics GPP1001V0M-HCO PP
LyondellBasell Hostacom™ GP622 Polypropylene Homopolymer
Avient Maxxam™ FR PP 402 Polypropylene

PMO420 / 53629

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.