MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH50
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.

Technyl A 216 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical properties. This grade is used in automotive industry, manufacture of components of electrical tools, and transport and building.

This product is available in natural, black and in a wide range of standard colors.

Information provided by Rhodia; Rhodia has been acquired by Solvay.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Key Words: Polyamide 66; PA66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ISO 1183-A
Water Absorption 0.80 %0.80 %(Beginning Dry) 24 hours in water 23°C. ISO 62
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/inRHODIA-EP
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inRHODIA-EP
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 135 MPa19600 psiISO 527
Tensile Strength, Yield 135 MPa19600 psiISO 527
Elongation at Break 4.0 %4.0 %ISO 527
Tensile Modulus 7.50 GPa1090 ksiISO 527
Flexural Yield Strength 176 MPa25500 psiISO 178
Flexural Modulus 5.90 GPa856 ksiISO 178
Izod Impact Resistance 1.60 J/cm²7.61 ft-lb/in²ISO 180
Charpy Impact Unnotched 9.50 J/cm²45.2 ft-lb/in²ISO 179/EU-1993
Charpy Impact, Notched 1.60 J/cm²7.61 ft-lb/in²ISO 179/1EA-1993
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 2.00e+13 ohm-cm2.00e+13 ohm-cmIEC 93
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 93
Dielectric Constant 4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
IEC 250
Dielectric Strength 30.0 kV/mm762 kV/inIEC 243-1
Dissipation Factor 0.11
@Frequency 1e+6 Hz
0.11
@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 600 V600 VIEC 112
 
Thermal PropertiesMetricEnglishComments
Melting Point 263 °C505 °FISO 3146-C
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 260 - 270 °C500 - 518 °F
Middle Barrel Temperature 270 - 280 °C518 - 536 °F
Front Barrel Temperature 280 - 290 °C536 - 554 °F
Nozzle Temperature 271 - 279 °C520 - 535 °F
Melt Temperature 270 - 300 °C518 - 572 °F
Mold Temperature 80.0 - 120 °C176 - 248 °FSurface
Drying Temperature 80.0 °C176 °FDehumidifying Dryer
Dry Time 3 - 4 hour3 - 4 hour
Moisture Content <= 0.20 %<= 0.20 %
Back Pressure 0.138 - 0.345 MPa20.0 - 50.0 psi
Fill Speed 200 - 300 mm/sec7.87 - 11.8 in/secPeripheral Screw Speed
 
Descriptive Properties
Injection Speed (cm3/sec)120 - 170 cm3/sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH0
Domo Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH50
Domo Technyl® A 218 V35 Nylon 66, 35% Glass Fiber, EH50
Domo Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH0
Domo Technyl® A 218 V35 Nylon 66, 35% Glass Fiber, EH0

PRHO03 / 65931

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.