MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Beryllia, 99.5%; BeO
Categories: Ceramic; Oxide

Material Notes:

Key Words: Beryllium Oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.85 g/cc0.103 lb/in³
a Lattice Constant 2.698 Å2.698 Å
c Lattice Constant 4.38 Å4.38 Å
 
Mechanical PropertiesMetricEnglishComments
Poissons Ratio  0.34
@Temperature 20.0 - 1000 °C
0.34
@Temperature 68.0 - 1830 °F
 0.38
@Temperature 20.0 °C
0.38
@Temperature 68.0 °F
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 6.5
@Frequency 1e+6 Hz
6.5
@Frequency 1e+6 Hz
Dissipation Factor 0.00040
@Frequency 1e+6 Hz
0.00040
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 2844 J/g1223 BTU/lb
CTE, linear  6.40 µm/m-°C
@Temperature 200 °C
3.56 µin/in-°F
@Temperature 392 °F
 7.20 µm/m-°C
@Temperature 500 °C
4.00 µin/in-°F
@Temperature 932 °F
Thermal Conductivity 248 W/m-K1720 BTU-in/hr-ft²-°F
 188 W/m-K
@Temperature 100 °C
1300 BTU-in/hr-ft²-°F
@Temperature 212 °F
Melting Point 2527 °C4581 °F
 
Descriptive Properties
Crystal StructureHexagonalWurtzite (Zincite) Structure - Space Group P 63mc

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Beryllium Oxide, BeO (Bromellite)
Materion Thermalox® 995 General Purpose 99.5% BeO
Beryllium, Be
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3
Overview - Alumina, 98%, Al2O3

BBeOA / 148

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.