MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay CYCOM® 890 RTM Epoxy Neat Resin
Categories: Polymer; Thermoset; Epoxy

Material Notes: CYCOM® 890 RTM is a one-part liquid epoxy resin system. It has one month out-life at room temperature which reduces the time required for the freeze-thaw-storage processes in a production environment. Its frozen storage shelf-life is 12 months at -18°C (0°F). CYCOM 890 RTM’s viscosity is low enough at 80°C (175°F) to allow injection without excessive heating of either the resin or the transfer pipework. When the resin is heated to cure temperature its viscosity is further reduced, helping to ensure full wet-out of the reinforcing fibers. CYCOM 890 RTM is fully cured after two hours at 180°C (355°F) after which it will have a continuous dry service performance of 170°C (338°F) and a continuous hot/wet service performance of 160°C (320°F) If needed, an optional free-standing postcure for two hours at 200°C (390°F) can be used. After postcure the resin will have a continuous dry service performance of 195°C (383°F) and a continuous hot/wet service performance of 170°C (338°F). CYCOM 890 RTM is compatible with the range of reinforcing fibers used in manufacturing composite components, i.e., carbon, glass, aramid, etc. A fully compatible binder system, CYCOM® 7720 has been developed for use with CYCOM 890 RTM. The binder is available pre-coated onto fabric. A separate datasheet for CYCOM 7720 is available on request.

Features & Benefits:

  • One-part system
  • 30 day out-life at room temperature
  • 12 month shelf-life at -18°C (0°F)
  • Injectable at 80°C (175°F) with a 24-hour pot-life
  • 250 cps initial injection viscosity
  • Less than 10 cps minimum viscosity
  • Two hours at 180°C (355°F) cure
  • 170°C (350°F) continuous dry service performance [195°C (383°F) after optional post-cure]
  • 160°C (320°F) continuous hot/wet service performance [170°C (338°F) after optional post-cure]
  • Fully compatible with CYCOM 7720 binder coating and CYCOM® 890-1 low resin content (LRC) filmfor tack enhancing fabrics
  • Low reactivity; No special shipping requirements
Applications: Infusion applications requiring low viscosity and extended pot-life
  • Control surfaces
  • Nacelle casing
  • Large surface fairings
  • Hinges/brackets/fittings

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 68.9 MPa10000 psi
Elongation at Break >= 6.3 %>= 6.3 %
Tensile Modulus 3.10 GPa450 ksi
Flexural Strength 136 MPa19700 psi
Flexural Modulus 3.20 GPa464 ksi
Flexural Strain at Break >= 3.3 %>= 3.3 %
Fracture Toughness 0.900 MPa-m½0.819 ksi-in½
Shear Modulus  1.13 GPa
@Temperature 93.0 °C
164 ksi
@Temperature 199 °F
 1.20 GPa
@Temperature 82.0 °C
174 ksi
@Temperature 180 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 170 °C338 °Fwet
 195 °C383 °Fdry
Glass Transition Temp, Tg 169 °C336 °FE' onset, 48 hr water boil
 191 °C376 °FE' onset
 210 °C410 °Fpeak tan delta
 210 °C410 °Fpeak tan delta, wet, 48 hr water boil
 
Processing PropertiesMetricEnglishComments
Processing Temperature 179 °C
@Time 7200 sec
355 °F
@Time 2.00 hour
Cure
Shelf Life 12.0 Month
@Temperature -17.8 °C
12.0 Month
@Temperature 0.000 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay CYCOM® PR 520 RTM Resin System
DuPont™ Kevlar® 29 Aramid Fiber
Solvay CYCOM® 823 RTM Liquid Epoxy Resin
Teijin Technora® Aramid Fiber
Röchling GoldMember™ Pre-tensioned Fiber Reinforcements

PCYTED087 / 180389

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.