MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos Styrenics 495F High-Impact Polystyrene Resin (Global)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Description: High-impact, high-flow grade for a wide variety of applications, including appliance components, consumer electronics housings, magnetic and optical media, building and construction, packaging and food service, recreation equipment and sporting goods, medical devices and labware, office products, cosmetic and personal care products, and housewares.

Information provided by BASF.


Ineos Styrenics purchased this product line from BASF in 2005.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM D792
Moisture Absorption at Equilibrium <= 0.10 %<= 0.10 %23°C/50% RH
Water Absorption at Saturation <= 0.10 %<= 0.10 %
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D955
Melt Flow 8.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
8.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 5555ASTM D785
Tensile Strength at Break 20.0 MPa2900 psiASTM D638
Tensile Strength, Yield 21.0 MPa3050 psiASTM D638
Elongation at Break 55 %55 %ASTM D638
Tensile Modulus 2.137 GPa310.0 ksiASTM D638
Flexural Modulus 1.655 GPa240.0 ksiASTM D790-1
Izod Impact, Notched 1.23 J/cm2.30 ft-lb/inASTM D256-A
Gardner Impact 31.6 J
@Thickness 3.17 mm,
Temperature 23.0 °C
23.3 ft-lb
@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D3029
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C174 °FASTM D648
Vicat Softening Point 97.0 °C207 °FASTM D1525
Flammability, UL94  HB
@Thickness 1.62 mm
HB
@Thickness 0.0638 in
HB CSA 0.6, All Colors
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
HB UL94, All Colors
 
Optical PropertiesMetricEnglishComments
Gloss 45 %45 %60°; ASTM D523
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 280 °C356 - 536 °FMolding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution PS 495F HIPS
INEOS Styrolution Polystyrol 495 F GR 2 PS
Overview of materials for Polystyrene, Impact Modified
ALM PS 200 Prototyping Polymer
Ineos Nova 4300 High Impact Polystyrene

PSG103 / 67264

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.