MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Saint-Gobain Tygon® S3™ B-44-3 Bio-based Beverage Tubing Formulation
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic

Material Notes: Tygon S3™ B-44-3, from Saint-Gobain Performance Plastics, is now phthalate-free. Saint-Gobain is proud to be among the first companies to offer sustainable flexible tubing products. The bio-based Tygon S3™ line combines the high performance standards customers demand with an eco-friendly tubing design.

Tygon S3™ Beverage Tubing is specially formulated for transferring a wide variety of beverages including soft drinks, fruit juices, flavored teas and bottled water. In virtually all cases, Tygon S3™ Beverage Tubing will not affect the taste or odor of product transferred through it, while its excellent non-wetting properties facilitate complete drainage and permit simple flush-cleaning.

Many of the properties inherent to Tygon S3™ Beverage Tubing also apply to a wide variety of complex applications ranging from fine cosmetic production to the dispensing of water-based printing inks found in the publishing industry. The versatility and proven performance of Tygon S3™ Beverage Tubing have made it a widely specified clear, flexible plastic tubing.

Features and Benefits

  • Clear as glass for easy visual monitoring of flow
  • Lightweight and flexible for easy, quick installation
  • Broad chemical resistance
  • Non-wetting properties allow easy
  • Cleaning and complete drainage
  • Contains no BPA or phthalates

Regulatory Compliance: This product is complies with FDA, 3A, and NSF standards in the US and Reach, 1935/2004/EC, and 10/2011/EU standards in the EU.

Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D792
Water Absorption 0.22 %
@Temperature 22.8 °C,
Time 86400 sec
0.22 %
@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 66
@Time 15.0 sec
66
@Time 0.00417 hour
ASTM D2240
Tensile Strength 15.2 MPa2200 psiASTM D412
Tensile Stress at Strain 9.508 MPa
@Strain 200 %
1379 psi
@Strain 200 %
Elongation at Break 390 %390 %ASTM D412
Tear Strength 43.8 kN/m250 pliASTM D1004
Compression Set 59 %
@Temperature 70.0 °C,
Time 79200 sec
59 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395 Method B
Tensile Set 57 %57 %at 75% Elongation; ASTM D412
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 73.9 °C165 °F
Minimum Service Temperature, Air -67.0 °C-88.6 °Ftemperature limit for flexibility
Brittleness Temperature -35.6 °C-32.0 °FASTM D746
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %Clear, but value not quantified
 
Compliance PropertiesMetricEnglishComments
European Food 1935/2004 YesYes
FDA YesYes
NSF YesYes
 
Descriptive Properties
ColorClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Tygon® S3™ E-3603 Phthalate-free Vacuum and Laboratory Tubing
Saint-Gobain Tygon® S3™ B-44-4X Phthalate-free Food, Milk, and Dairy tubing
Overview of materials for Polyphenylene Sulfide (PPS); Molded
Saint-Gobain Tygon® LP 1100 Low Permeation Fuel Tubing
Saint-Gobain Versilon ™ Silver Antimicrobial Tubing

PSTGQ902 / 160398

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.