MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cossa Polimeri ESTABLEND 6500 Polycarbonate ABS Blend
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: Polycarbonate and Acrylonitrile Butadiene Styrene blend

High thermal resistance, high impact resistance

Information provided by Cossa Polimeri S.r.l.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ASTM D 792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D 955
Melt Flow 20 g/10 min
@Load 5.00 kg,
Temperature 260 °C
20 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 47.0 MPa6820 psiASTM D 638
Tensile Strength, Yield 59.0 MPa8560 psiASTM D 638
Elongation at Break >= 50 %>= 50 %ASTM D 638
Flexural Modulus 2.30 GPa334 ksiASTM D 790
Izod Impact, Notched  4.70 J/cm
@Temperature 0.000 °C
8.81 ft-lb/in
@Temperature 32.0 °F
ASTM D 638
 5.00 J/cm
@Temperature 23.0 °C
9.37 ft-lb/in
@Temperature 73.4 °F
ASTM D 256
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point  125 °C
@Load 5.00 kg
257 °F
@Load 11.0 lb
50°C/hr; ASTM D 1525
 135 °C
@Load 0.999 kg
275 °F
@Load 2.20 lb
50°C/hr; ASTM D 1525
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
Glow Wire Test 750 °C
@Thickness 2.00 mm
1380 °F
@Thickness 0.0787 in
I.E.C. 695-2-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chase Plastics CP Pryme® PCA100 Polycarbonate/ABS Alloy
Arkema OREVAC® 18390 Maleic Anhydride Modified Polyethylene
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
A. Schulman Diamond NYLON 6615 Black, Super Tough
Ineos ABS Lustran® 1148 General Purpose, High-Impact

PCOSSA852 / 156442

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.