MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

321 Stainless Steel, annealed plate
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Similar to Type 304 except Ti content helps prevent chromium carbide precipitation resulting from welding or elevated temperatures. Stabilized at annealing temperatures between 950-1010°C (1750-1850°F). Resists scaling and vibration fatigue. Applications include aircraft exhaust stacks and manifolds, chemical processing equipment, weld equipment, jet engine parts.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.00 g/cc0.289 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 150150
Hardness, Knoop 170170Converted from Brinell
Hardness, Rockwell B 8080
Hardness, Vickers 157157Converted from Brinell
Tensile Strength, Ultimate 585 MPa84800 psi
Tensile Strength, Yield 240 MPa34800 psi
Elongation at Break 55 %55 %in 50 mm
Modulus of Elasticity 193 - 200 GPa28000 - 29000 ksi
Izod Impact 135 J99.6 ft-lb
Charpy Impact 165 J122 ft-lb
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000720 ohm-cm0.0000720 ohm-cmat 20ºC
Magnetic Permeability 1.0081.008at RT
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.7 µm/m-°C
@Temperature 0.000 - 100 °C
9.28 µin/in-°F
@Temperature 32.0 - 212 °F
 17.1 µm/m-°C
@Temperature 0.000 - 315 °C
9.50 µin/in-°F
@Temperature 32.0 - 599 °F
 18.5 µm/m-°C
@Temperature 0.000 - 540 °C
10.3 µin/in-°F
@Temperature 32.0 - 1000 °F
 20.5 µm/m-°C
@Temperature 20.0 - 925 °C
11.4 µin/in-°F
@Temperature 68.0 - 1700 °F
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
0.120 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity 16.1 W/m-K
@Temperature 100 °C
112 BTU-in/hr-ft²-°F
@Temperature 212 °F
Melting Point 1400 - 1425 °C2550 - 2597 °F
Solidus 1400 °C2550 °F
Liquidus 1425 °C2597 °F
Maximum Service Temperature, Air 870 °C1600 °FContinuous Service
 925 °C1700 °FIntermittent
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.080 %<= 0.080 %
Chromium, Cr 17 - 19 %17 - 19 %
Iron, Fe 65.45 - 73.6 %65.45 - 73.6 %As Balance
Manganese, Mn <= 2.0 %<= 2.0 %
Nickel, Ni 9.0 - 12 %9.0 - 12 %
Phosphorus, P <= 0.045 %<= 0.045 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %
Titanium, Ti 0.40 %0.40 %Minimum Ti content = 5 x Carbon content

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
321 Stainless Steel, annealed bar
321 Stainless Steel, annealed sheet
321 Stainless Steel, annealed strip
304 Stainless Steel
347 Stainless Steel, annealed, plate

MQ321C / 12817

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.