MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Erbslöh Aluminium DISPAL S220 Aluminum Alloy, AlSi35, Condition F
Categories: Metal; Nonferrous Metal; Aluminum Alloy

Material Notes: Excellent properties:
  • abrasive stability
  • high stiffness (E-modulus)
  • resistance even at high temperatures
  • good grindability

PEAK DISPAL materials allow the manufacturing of pistons for highest operational demands.

Information provided by PEAK Werkstoff GmbH, a part of Erbslöh Aluminium GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.413 - 2.667 g/cc0.08718 - 0.09635 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers >= 65>= 65HV30
Tensile Strength at Break  >= 128 MPa
@Temperature 150 °C
>= 18600 psi
@Temperature 302 °F
 >= 165 MPa
@Temperature 20.0 °C
>= 23900 psi
@Temperature 68.0 °F
Tensile Strength, Yield  >= 76.0 MPa
@Temperature 150 °C
>= 11000 psi
@Temperature 302 °F
 >= 95.0 MPa
@Temperature 20.0 °C
>= 13800 psi
@Temperature 68.0 °F
Elongation at Break  >= 2.5 %
@Temperature 20.0 °C
>= 2.5 %
@Temperature 68.0 °F
 >= 8.4 %
@Temperature 150 °C
>= 8.4 %
@Temperature 302 °F
Modulus of Elasticity  >= 76.0 GPa
@Temperature 150 °C
>= 11000 ksi
@Temperature 302 °F
 >= 85.0 GPa
@Temperature 20.0 °C
>= 12300 ksi
@Temperature 68.0 °F
Poissons Ratio  0.275
@Temperature 20.0 °C
0.275
@Temperature 68.0 °F
 0.278
@Temperature 100 °C
0.278
@Temperature 212 °F
 0.28
@Temperature 150 °C
0.28
@Temperature 302 °F
 0.282
@Temperature 200 °C
0.282
@Temperature 392 °F
 0.284
@Temperature 250 °C
0.284
@Temperature 482 °F
 0.284
@Temperature 300 °C
0.284
@Temperature 572 °F
Shear Modulus  33.0 GPa
@Temperature 250 °C
4790 ksi
@Temperature 482 °F
 33.0 GPa
@Temperature 300 °C
4790 ksi
@Temperature 572 °F
 34.0 GPa
@Temperature 200 °C
4930 ksi
@Temperature 392 °F
 35.0 GPa
@Temperature 100 °C
5080 ksi
@Temperature 212 °F
 35.0 GPa
@Temperature 150 °C
5080 ksi
@Temperature 302 °F
 36.0 GPa
@Temperature 20.0 °C
5220 ksi
@Temperature 68.0 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000620 - 0.00000660 ohm-cm0.00000620 - 0.00000660 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  14.6 - 15.6 µm/m-°C
@Temperature 20.0 - 100 °C
8.11 - 8.67 µin/in-°F
@Temperature 68.0 - 212 °F
 15.5 - 16.5 µm/m-°C
@Temperature 20.0 - 200 °C
8.61 - 9.17 µin/in-°F
@Temperature 68.0 - 392 °F
 16.3 - 17.3 µm/m-°C
@Temperature 20.0 - 300 °C
9.06 - 9.61 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.830 - 0.870 J/g-°C0.198 - 0.208 BTU/lb-°F
Thermal Conductivity  123.5 W/m-K
@Temperature 400 °C
857.1 BTU-in/hr-ft²-°F
@Temperature 752 °F
 131 W/m-K
@Temperature 300 °C
909 BTU-in/hr-ft²-°F
@Temperature 572 °F
 136.8 W/m-K
@Temperature 200 °C
949.4 BTU-in/hr-ft²-°F
@Temperature 392 °F
 144.3 W/m-K
@Temperature 100 °C
1001 BTU-in/hr-ft²-°F
@Temperature 212 °F
 152.4 W/m-K
@Temperature 30.0 °C
1058 BTU-in/hr-ft²-°F
@Temperature 86.0 °F
Melting Point 573 - 881 °C1060 - 1620 °F
Solidus 572.9 - 578.9 °C1063 - 1074 °F
Liquidus 875.3 - 881.3 °C1608 - 1618 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 65 %65 %As Balance
Silicon, Si 35 %35 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Erbslöh Aluminium DISPAL S220 Aluminum Alloy, AlSi35, Condition O
Erbslöh Aluminium DISPAL S225 Aluminum Alloy, AlSi35Fe2Ni, Condition F
Erbslöh Aluminium DISPAL S226 Aluminum Alloy, AlSi30CuMg, Condition T6
Erbslöh Aluminium DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6x
Erbslöh Aluminium DISPAL S230 Aluminum Alloy, AlSi17Fe5Cu4Mg

NPEAK01a / 170254

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.