MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ovako 51CrV4 EN10089:2002 Steel, Tempering
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: General Information: 51CrV4 is a high strength quench and tempering steel suitable for quenched and tempered springs. What Ovako offer includes a number of variants with tight chemical composition, suitable for different applications and material thicknesses. They all meet the overall requirements set by EN10089.
Variant SB9292 is a strong variant with hardenability in the upper part of the +HH band and low content of non-metallic inclusions.
Variant SB9290 has somewhat lower hardenability, but is still strong.
Variant SB9282 has medium hardenability and is a good start for applications with normal requirements.
Variant SB9212 which has a good surface hardness, but it will not through harden for thicker dimensions. It is instead a god pick for thin sections.
Variants Ovako 593B and 593Q are also mainly used for springs, but frequently used for shafts and machine components.
Ovako 593Q is an IQ (isotropic quality) variant.

IQ-Steel®IQ-Steel® is an isotropic quality ultra clean steel optimized for high fatigue strength under multi axial loading.

Information provided by Ovako

Key Words: WNr 1.8159, 735A51, SS2230, SB9292 - 52CrMn5-4, SB9290 - 52CrMn5-4, SB9282 - 52CrMn4-4, SB9212- 50CrMn4-4
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 1350 - 1650 MPa196000 - 239000 psiAll formats
Tensile Strength, Yield >= 1200 MPa>= 174000 psiAll formats
Elongation at Break 6.0 %6.0 %All formats
Reduction of Area 30 %30 %All formats
Modulus of Elasticity 210 GPa30500 ksi
Poissons Ratio 0.300.30
Shear Modulus 80.0 GPa11600 ksi
Impact Test 8.00 J5.90 ft-lbAll formats, long
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
6.67 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
0.110 - 0.115 BTU/lb-°F
@Temperature 122 - 212 °F
Thermal Conductivity 40.0 - 45.0 W/m-K278 - 312 BTU-in/hr-ft²-°FAmbient temperature
Transformation Temperature 273 °C523 °FMS
 738 °C1360 °FAC1
 778 °C1430 °FAC3
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.47 - 0.55 %0.47 - 0.55 %
Chromium, Cr 0.90 - 1.2 %0.90 - 1.2 %
Iron, Fe 96.7 - 97.93 %96.7 - 97.93 %As Balance
Manganese, Mn 0.70 - 1.1 %0.70 - 1.1 %
Phosphorus, P <= 0.025 %<= 0.025 %
Silicon, Si <= 0.40 %<= 0.40 %
Sulfur, S <= 0.025 %<= 0.025 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rene 62 Superalloy
Ovako 51CrV4 SB9292 Steel, Tempering
Ovako 51CrV4 SB9290 Steel, Tempering
Ovako 51CrV4 SB9212 Steel, Hot forging
Ovako 51CrV4 EN10089:2002 Steel, AC

NOVAKO343 / 234642

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.