MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bi48-Pb28.5-Sn14.5 Bismuth-Lead-Tin Fusible Alloy
Categories: Metal; Nonferrous Metal; Bismuth Alloy

Material Notes: Noneutectic fusible alloy with a low melting temperatureApplications:
  • Matrix metal for punch and die assemblies and small bearings
  • Anchoring
  • Punch and Die applications

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 9.50 g/cc9.50 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 2222
Tensile Strength 90.0 MPa13100 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000670 ohm-cm0.0000670 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Melting Point 103 - 227 °C217 - 441 °F
Solidus 103 °C217 °F
Liquidus 227 °C441 °F
 
Component Elements PropertiesMetricEnglishComments
Antimony, Sb 9.0 %9.0 %
Bismuth, Bi 48 %48 %
Lead, Pb 28.5 %28.5 %
Tin, Sn 14.5 %14.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bi48-Pb25.63-Sn12.77-Cd9.6 Bismuth-Lead-Tin-Cadmium Fusible Alloy
Bi50-Pb34.5-Sn9.3-Cd6.2 Bismuth-Lead-Tin-Cadmium Fusible Alloy; von Hauer's Alloy II
Bi50.5-Pb27.8-Sn12.4-Cd9.3 Bismuth-Lead-Tin-Cadmium Fusible Alloy
AIM 47 Fusible Bismuth Alloy
Bi33-Pb33-Sn33 Bismuth-Lead-Tin Fusible Alloy, Homsberg's Alloy, UNS L54835

MLBIS941 / 135555

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.