MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Mylar® 75 OL Polyester Film, 75 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Data provided by DuPont Packaging Polymers.

An exceptionally strong polyester film designed to package foods. The film is suitable for heating food products in microwave or conventional ovens. Can be used to package, distribute, and heat foods up to 204°C (400°F).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³Average value for Mylar® films.
Moisture Vapor Transmission 0.600 cc-mm/m²-24hr-atm1.52 cc-mil/100 in²-24hr-atmASTM 1249
Water Vapor Transmission 30.0 g/m²/day1.93 g/100 in²/dayASTM 1249
Oxygen Transmission 2.10 cc-mm/m²-24hr-atm5.33 cc-mil/100 in²-24hr-atmor 110 cc/m²-24hr-atm for the film. ASTM D3985
Thickness 19.0 microns0.750 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 130 %130 %ASTM D882
Film Elongation at Break, TD 100 %100 %ASTM D882
Modulus of Elasticity 3.79 GPa550 ksi(stiffness), ASTM D882
Tear Strength Test 400400Graves, g; ASTM D1004
Seal Strength 247 g/25 mm247 g/in
Film Tensile Strength at Break, MD 200 MPa29000 psiASTM D882
Film Tensile Strength at Break, TD 242 MPa35100 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C399 °FFoods can be heated or cooked up to this temperature.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® 50 OL Polyester Film, Ovenable Lidding, Heat Sealable, 50 Gauge
DuPont Teijin Films Mylar® HS Polyester Film, 48 Gauge (12 µm)
DuPont Teijin Films Mylar® LB Polyester Film, 48 Gauge (12 µm)
DuPont Teijin Films Mylar® M34 Polyester Film, 50 Gauge (13 µm), PVDC Coated
DuPont Teijin Films Mylar® A Polyester Film, 1400 Gauge

PDU670 / 33119

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.