MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® A 225F PA66, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Description: Unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for very fast cycles.

Available in: Europe, Latin America and North America

Product Applications: TECHNYL ® A 225F offers two main advantages excellent filling qualities and UL 94 V2 under 0.4 mm. It is particularly used in electrical applications to mould parts with a good dimensional stability, such as: Unfilled bobbin coil forers for electrical motors, Transformers, and Connectors. This product is available in natural.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183/A
Water Absorption 1.1 %
@Temperature 23.0 °C,
Time 86400 sec
1.1 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.0083 cm/cm0.0083 in/inIsotropy
Linear Mold Shrinkage, Flow 0.015 cm/cm0.015 in/in
Linear Mold Shrinkage, Transverse 0.018 cm/cm0.018 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 70.0 MPa10200 psiISO 527 Type 1A
Tensile Strength, Yield 85.0 MPa12300 psiISO 527 type 1 A
Elongation at Break 20 %20 %ISO 527 Type 1A
Elongation at Yield 5.0 %5.0 %ISO 527 type 1 A
Tensile Modulus 3.20 GPa464 ksiISO 527 Type 1A
Flexural Strength 125 MPa18100 psiISO 178
Flexural Modulus 3.15 GPa457 ksiISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²ISO 180/1eA
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.00e+15 ohm-cm4.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
Dielectric Constant 2.92.9IEC 60250
Dielectric Strength 27.0 kV/mm686 kV/inIEC 60243
Dissipation Factor 0.0200.020IEC 60250
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
36.1 µin/in-°F
@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 263 °C505 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FISO 75/Af
Flammability, UL94  V-2
@Thickness 0.380 mm
V-2
@Thickness 0.0150 in
1210
 V-2
@Thickness 0.800 mm
V-2
@Thickness 0.0315 in
1210
 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
1210
Glow Wire Flammability Index 960 °C1760 °FISO 60695-2-12
 
Processing PropertiesMetricEnglishComments
Feed Temperature 250 - 280 °C482 - 536 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone260-290°C
Mixing Zone270-300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES HiFill® PA4/6 0206
Domo Technyl® A218 Heat Stabilized Nylon 66
Domo Technyl® A 205F Nylon 66, EH0
Techmer ES HiFill® PA4/6 HS LBK
Domo TECHNYL® 2210HS PA66, Conditioned

PRHOD689 / 137920

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.