MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChevronTexaco Delo® NLGI 00 Grease EP
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Features

Chevron Delo Greases EP are technically advanced, extreme pressure greases for a wide variety of on- and off-road applications.

They are formulated with ISOSYN® base stocks, a lithium complex thickener, rust and oxidation inhibitors, and extreme pressure and tackiness additives. They are blue in color with a tacky texture. They are engineered to minimize friction and wear with a thick, velvety coating for excellent load carrying protection.

Chevron Delo Greases EP are specially formulated for extreme pressure wheel bearing and chassis applications including the steering drag links, king pins, transmission cross shaft spring pins, shackle pins, brake cam shafts, and fifth wheel faceplates and pivots operating under high and low temperature conditions. The high viscosity index base oil makes these products perfect for the centralized lubrication systems found on today`s mobile equipment.

These products are formulated to perform in unusually demanding conditions of high and low temperatures. The lithium complex thickener in Chevron Delo Greases EP elevates the dropping point to approximately 266°C (510°F). This high dropping point equates to excellent high temperature stability up to 177°C (350°F). Chevron Delo Greases EP have the proper base oil viscosity to meet NLGI GC-LB requirements for low temperature operation. NLGI 1 and 2 are recommended for applications operating in the temperature range of -18°C to 177°C (0°F to 350°F). NLGI 00 and 0 can be used at temperatures as low as -34°C (-30°F).

Chevron Delo Greases EP exceed the requirements of NLGI GC-LB for EP protection and rust protection, making them well suited for the most severe applications.

Applications

Chevron Delo Greases EP are designed for extreme duty in a wide variety of on- and off-highway vehicle and equipment applications.

On-highway heavy duty trucks — These lubricants are perfect for a wide variety of Class 8 trucks in all chassis and wheel bearing applications ranging from automatic centralized greasing systems to wheel bearings operating near the high temperatures of disc brakes. This product is for all applications, from owner/operators to fleets (especially those considering extended service intervals).

Off-highway vehicles — Whether the application is in construction, logging, mining, agriculture or utilities, these greases will perform. Use them in haul trucks, loaders, tractors, cherry pickers or any of a number of other off-highway vehicles.

Medium- and light-duty trucks and buses —As with their heavy duty counterparts, the Class 7 and Class 6 vehicles and buses require an extreme duty grease. Chevron Delo Greases EP will provide that performance.

Automobiles — Chevron Delo Greases EP are exceptional lubricants for high temperature wheel bearings and other high performance automotive applications.

NLGI 1 and 2 are approved for the NLGI Certification Mark GC-LB. Chevron Delo Greases EP meet the requirements of the Mack MG-C grease specification.

Key Words: CPS Number: 235212; MSDS Number: 6818
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 100100Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 992 SUS992 SUS
Saybolt Viscosity at 210°F 90 SUS90 SUS
Kinematic Viscosity at 40°C (104°F) 189 cSt189 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 17.5 cSt17.5 cStASTM D445
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 400 kg882 lb (mass)Weld Point
Four Ball Wear 0.450 mm0.0177 in
Penetration 415415Worked (60 strokes)
Penetration P(0), 1/10 mm 430430
Timken Test 24900 g55.0 lb
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 77.0 °C171 °F
Minimum Service Temperature, Air -34.0 °C-29.2 °F
Flash Point 246 °C475 °FASTM D92
Dropping Point 235 °C455 °F
 
Descriptive Properties
Bearing RustPass
ColorBlue
Corrosion, Copper Strip Test 3h1B
Lincoln Ventmeter, psig at 30 s, at 0°F50
Lincoln Ventmeter, psig at 30 s, at -22°F100
Lincoln Ventmeter, psig at 30 s, at 30°F50
TextureTacky
Thickener, % / type4 / Lithium Complex

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ChevronTexaco Dura-Lith® NLGI 00 Grease EP
Overview of materials for AISI 4000 Series Steel
Mitsui MILEX™ RS-2210MB Silicone Rubber Modified Phenolic Resin
Dow Elvax® 550 Ethylene-Vinyl Acetate Copolymer Resin
Dow Elvax® 250 Ethylene-Vinyl Acetate Copolymer Resin

WCHEV243 / 74858

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.