MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik Vestamid® L-GF15 23% Glass Filled Nylon 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 20% Glass Fiber Filled

Material Notes: Description: 15% chopped strands, medium-viscosity, heat-stabilized, with processing aid

Applications: Gear box housing for electric car window lifts

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Key Words: PA12,MHR,16-040,GF15
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.60 %
@Thickness 1.00 mm,
Temperature 23.0 °C
0.60 %
@Thickness 0.0394 in,
Temperature 73.4 °F
50% R.H.; ISO 62
Water Absorption at Saturation 1.3 %
@Thickness 1.00 mm
1.3 %
@Thickness 0.0394 in
ISO 62
Linear Mold Shrinkage 0.0010 cm/cm0.0010 in/in127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)
Linear Mold Shrinkage, Transverse 0.011 cm/cm0.011 in/in127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 95.0 MPa13800 psiISO 527-1/2
Elongation at Break 6.0 %6.0 %ISO 527-1/2
Tensile Modulus 3.90 GPa566 ksiISO 527-1/2
Charpy Impact Unnotched  7.50 J/cm²
@Temperature 23.0 °C
35.7 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
 8.00 J/cm²
@Temperature -30.0 °C
38.1 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  1.10 J/cm²
@Temperature -30.0 °C
5.24 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.70 J/cm²
@Temperature 23.0 °C
8.09 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Dielectric Constant  3.4
@Frequency 1e+6 Hz
3.4
@Frequency 1e+6 Hz
IEC 60250
 4.0
@Frequency 100 Hz
4.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 44.0 kV/mm1120 kV/inK20/P50; IEC 60243-1
Dissipation Factor  0.026
@Frequency 1e+6 Hz
0.026
@Frequency 1e+6 Hz
IEC 60250
 0.038
@Frequency 100 Hz
0.038
@Frequency 100 Hz
IEC 60250
Comparative Tracking Index >= 600 V>= 600 VTest Solution A, 50 drops; IEC 60112
 600 V600 VTest Solution A, 100 drops; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 131 °F
45x15x10 mm; ISO 11359
Melting Point 178 °C352 °FPeak Temperature; ISO 3146, ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 175 °C347 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 160 °C320 °FISO 75
Vicat Softening Point 170 °C338 °F50N; ISO 306
 175 °C347 °F10N; ISO 306
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 V-2
@Thickness 3.20 mm
V-2
@Thickness 0.126 in
 
Descriptive Properties
Electrolytic CorrosionA1 StepIEC 60426

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik Vestamid® L1833 30% Glass Filled Nylon 12
Evonik Vestamid® L-GF30 30% Glass Filled Nylon 12
Arkema Rilsamid® AECHVO TL PA12
Evonik Vestamid® L1930 30% Glass Bead Filled Nylon 12
Covestro Makrolon® Rx2530 Polycarbonate

PHULA45 / 47405

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.