MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 7039-O
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 7000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A97039; Aluminium 7039-O; AA7039-O; Al7039-O
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.74 g/cc0.0990 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 6161500 kg load with 10 mm ball
 61
@Load 1500 kg
61
@Load 3310 lb
Hardness, Knoop 8282Converted from Brinell Hardness Value
Hardness, Vickers 6969Converted from Brinell Hardness Value
Tensile Strength, Ultimate 227 MPa32900 psiLongitudinal
 227 MPa32900 psiTransverse
 230 MPa33400 psi
Tensile Strength, Yield 100 MPa14500 psi
 103 MPa14900 psiLongitudinal; 0.2%
 103 MPa14900 psiTransverse; 0.2%
Elongation at Break 22 %22 %Longitudinal
 22 %22 %Transverse
 22 %
@Thickness 1.60 mm
22 %
@Thickness 0.0630 in
In 5 cm
Modulus of Elasticity 69.6 GPa10100 ksiAverage of Tension and Compression. In Al alloys, the compressive modulus is typically 2% greater than the tensile modulus
Poissons Ratio 0.330.33Estimated from trends in similar Al alloys.
Shear Modulus 26.0 GPa3770 ksiEstimated from similar Al alloys.
Shear Strength 140 MPa20300 psiCalculated value.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000450 ohm-cm0.00000450 ohm-cmEstimated from trends in similar Al alloys.
 
Thermal PropertiesMetricEnglishComments
CTE, linear  23.4 µm/m-°C
@Temperature 20.0 - 100 °C
13.0 µin/in-°F
@Temperature 68.0 - 212 °F
 25.2 µm/m-°C
@Temperature 20.0 - 300 °C
14.0 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.880 J/g-°C0.210 BTU/lb-°FEstimated from trends in similar Al alloys.
Thermal Conductivity 140 W/m-K972 BTU-in/hr-ft²-°F
Melting Point 482 - 638 °C900 - 1180 °F
Solidus 482 °C900 °F
Liquidus 638 °C1180 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 354 - 371 °C670 - 700 °F
 413 - 454 °C775 - 850 °Fsoak for 2-3 hr, air cool, reheat at 450°F, hold at temperature for 4 hr, air cool; or heat to 670 to 700°F, air cool
Solution Temperature 460 - 499 °C860 - 930 °Fsoak 2 hr, quench in cold water; sheet stock should be quenched from 910 to 930°F, while extruded stock should be quenched from 860 to 880°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 90.5 - 90.5 %90.5 - 90.5 %As remainder
Chromium, Cr 0.15 - 0.25 %0.15 - 0.25 %
Copper, Cu <= 0.10 %<= 0.10 %
Iron, Fe <= 0.40 %<= 0.40 %
Magnesium, Mg 2.3 - 3.3 %2.3 - 3.3 %
Manganese, Mn 0.10 - 0.40 %0.10 - 0.40 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.30 %<= 0.30 %
Titanium, Ti <= 0.10 %<= 0.10 %
Zinc, Zn 3.5 - 4.5 %3.5 - 4.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 7039-T64
Aluminum 7039-T61
Aluminum 5052-H32
Aluminum 7034-T6
Overview of materials for 7000 Series Aluminum Alloy

MA7039O / 9564

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.