MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® B 230 PA66/6, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66

Material Notes: Description: Unreinforced and modified copolyamide 66/6, with high flexibility and improved impact resistance, for injection molding.

Available in: Asia Pacific and Europe

Product Applications: TECHNYL ® B 230 is particularly recommended for applications where good impact resistance at low and room temperature is required , also for parts which could break during assembly or parts used at low humidity levels. This grade is commonly used in: automotive industry: bumpers and clips sports and leisure: sports bag buckles and electrical appliance: cable ties. This product is available in natural, black, and in colors on request.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ISO 1183/A
Water Absorption 1.35 %
@Temperature 23.0 °C,
Time 86400 sec
1.35 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.0107 cm/cm0.0107 in/inIsotropy
Linear Mold Shrinkage, Flow 0.022 cm/cm0.022 in/in
Linear Mold Shrinkage, Transverse 0.0205 cm/cm0.0205 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 50.0 MPa7250 psiISO 527 Type 1A
Tensile Strength, Yield 60.0 MPa8700 psiISO 527 type 1 A
Elongation at Break 50 %50 %ISO 527 Type 1A
Elongation at Yield 5.0 %5.0 %ISO 527 Type 1A
Tensile Modulus 2.30 GPa334 ksiISO 527 Type 1A
Flexural Strength 80.0 MPa11600 psiISO 178
Flexural Modulus 2.00 GPa290 ksiISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²3.33 ft-lb/in²ISO 180/1eA
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²3.81 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 5.00e+14 ohm5.00e+14 ohmIEC 60093
Dielectric Strength 20.0 kV/mm508 kV/inIEC 60243
Dissipation Factor 0.0200.020IEC 60250
Comparative Tracking Index 475 V475 VSolution B; IEC 60112
 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
38.9 µin/in-°F
@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 242 °C468 °FISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 185 °C365 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C144 °FISO 75/Af
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
1210
Oxygen Index 21 %21 %ISO 4589
 
Processing PropertiesMetricEnglishComments
Feed Temperature 245 - 255 °C473 - 491 °F
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone255-265°C
Mixing Zone265-275°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grilon® TSZ 1 PA666
Domo TECHNYL® B 238 Black 21 N PA66/6, DRY
Domo TECHNYL® B 216 Natural D PA66/6, DRY
Domo TECHNYL® B 230 PA66/6, Conditioned
Domo TECHNYL® B 218 Black 21 N PA66/6, DRY

PRHOD743 / 137974

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.