MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plastcom SLOVALEN PC 71 GF 10 PP, 10% glass fibre  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 10% Glass Fiber Filler

Material Notes: Features

Compouded homopolymer PP, with the content of 10% chemically bound glass fibre and modifier of mechanical properties. Increased strength in comparison with unfilled PP. Use in all industry sectors. Delivered in the natural mode and in the full RAL colour scale.

Packaging, transport, stocking

The product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.

Information Provided by Plastcom spol. s r.o.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³
Linear Mold Shrinkage 0.0144 cm/cm0.0144 in/in
Linear Mold Shrinkage, Transverse 0.0131 cm/cm0.0131 in/in
Melt Flow 12 g/10 min
@Load 0.325 kg,
Temperature 270 °C
12 g/10 min
@Load 0.716 lb,
Temperature 518 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 35.0 MPa5080 psi
Elongation at Break 6.0 %6.0 %
Tensile Modulus 2.80 GPa406 ksi
Flexural Strength 45.0 MPa6530 psi
Flexural Modulus 2.50 GPa363 ksi
Charpy Impact Unnotched  2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
 2.00 J/cm²
@Temperature -20.0 °C
9.52 ft-lb/in²
@Temperature -4.00 °F
Charpy Impact, Notched  0.500 J/cm²
@Temperature -20.0 °C
2.38 ft-lb/in²
@Temperature -4.00 °F
 0.600 J/cm²
@Temperature 23.0 °C
2.86 ft-lb/in²
@Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point 136 °C277 °F
Deflection Temperature at 1.8 MPa (264 psi) 130 °C266 °F
Vicat Softening Point 145 °C293 °FB
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 230 °C392 - 446 °F
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F
Injection Pressure 60.0 - 100 MPa8700 - 14500 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plastcom SLOVAMID 6 GF 20 PA6, 20% glass beads
Plastcom SLOVAMID 6 GF 10 TS PA6, 10% glass fibre
Plastcom SLOVAMID 6 GF 10 GB 20 PA6, 10% glass fibre
Plastcom SLOVALEN PQ 81 T 10 PP, 10% mineral filling
Omni Plastics OmniTech™ HDPE TF10 High Density Polyethylene, 10% Talc reinforced

PPLACO274 / 120898

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.