MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ethylene glycol, C2H6O2
Categories: Fluid; Solvent

Key Words: C2H6O2
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.114 g/cc
@Temperature 20.0 °C
0.04025 lb/in³
@Temperature 68.0 °F
Viscosity 18.376 cP
@Temperature 20.0 °C
18.376 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 62.069 g/mol62.069 g/mol
Vapor Pressure 0.000111 bar
@Temperature 20.0 °C
0.0830 torr
@Temperature 68.0 °F
Surface Tension 48.49 dynes/cm
@Temperature 20.0 °C
48.49 dynes/cm
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 77.0 bar57800 torr
Critical Temperature 372 °C702 °F
Critical Density 0.334 g/cc0.0121 lb/in³
Critical Molar Volume 186 cm³/mol11.4 in³/mol
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 37.7
@Temperature 20.0 °C
37.7
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 846 J/g364 BTU/lb
Specific Heat Capacity 2.433 J/g-°C0.5815 BTU/lb-°F
 1.565 J/g-°C
@Temperature 25.0 °C
0.3740 BTU/lb-°F
@Temperature 77.0 °F
Vapor
Thermal Conductivity 0.256 W/m-K
@Temperature 20.0 °C
1.78 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point -13.0 °C8.60 °F
Boiling Point 197.3 °C387.1 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.432
@Wavelength 589.3 nm
1.432
@Wavelength 589.3 nm
nD
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter20.2501
Antoine's Vapor Pressure B Parameter6022.18
Antoine's Vapor Pressure C Parameter-28.25
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)107-21-1
Chemical FormulaC2H6O2
Critical Compressibility (Zc)0.27
Dipole moment (p/C.m)7.338E-28
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A1365
Dynamic Viscosity Parameter B402.41
Henry's Law Constant (atm m3/mol)6E-08
Molar Heat Capacity (298K)97.157 J/mol-K
Molar Heat Capacity of Vapor a Parameter35.6728
Molar Heat Capacity of Vapor b Parameter0.2482
Molar Heat Capacity of Vapor c Parameter-0.0001496
Molar Heat Capacity of Vapor d Parameter3.008E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
UV cut-off (nm)210

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Du-Co Ceramics S-570 Silica
Quartz (SiO2)
Water, H2O
ChevronTexaco Havoline® SAE 10W-30 Synthetic Motor Oil
ChevronTexaco DEX-COOL® Extended Life Antifreeze/Coolant, Prediluted 50/50

VORGS173 / 99548

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.