MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Videolar-Innova 825 E High Impact Polystyrene (HIPS)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes:
  • Grade designed specially for extrusion and thermoforming
  • Characteristics make it especially suitable for industrial packaging deep draw thermoforming and custom multilayer sheet extrusion
Features:
  • Stress crack resistance
  • Good temperature resistance
Applications:
  • Refrigerator and packaging
  • Sheet, film and profile extrusion

Information provided by Dax Resinas

Key Words: FDA 21 CFR 177.1640
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.650 g/cc0.0235 lb/in³ISO 060
Density 1.04 g/cc0.0376 lb/in³ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/in
Melt Flow 3.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
3.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 23.0 MPa3340 psiASTM D638
Elongation at Yield 55 %55 %ASTM D638
Tensile Modulus 1.93 GPa280 ksiASTM D638
Flexural Strength 47.0 MPa6820 psiASTM D790
Flexural Modulus 2.14 GPa310 ksiASTM D790
Izod Impact, Notched 1.07 J/cm2.00 ft-lb/inASTM D256
Falling Dart Impact 14.0 J10.3 ft-lbASTM D5420
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C198 °F@ 264 psi; ASTM D648
Vicat Softening Point 99.0 °C210 °FASTM D1525
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Videolar-Innova 825 High Impact Polystyrene (HIPS)
Americas Styrenics EA6740 High Impact Polystyrene
Americas Styrenics EB6400 High Impact Polystyrene
Americas Styrenics Styron® 425 High Impact Polystyrene
Chevron Phillips EB6400 HIPS - High Impact Polystyrene

PDAX001 / 29426

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.