MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Vycom FLAMETEC™ CP5 Fire Retardant Polypropylene (FRPP)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Flametec™ CP5 was formulated to meet the SEMI S93 specification for fire safety in clean room applications. CP5 meets UL 94 V-0 fire classification and is extruded for gauge and dimensional consistency. CP5 has an excellent balance of physical properties, chemical resistance and fire safety.

FEATURES AND BENEFITS

  • Fire Retardant- Meets the SEMI S93 specification and UL 94 V-0.
  • Chemical Resistance- Resistance to a broad range of chemical processes.
  • Color- Bright White color for any clean room or laboratory equipment.
  • Fabrication- Cuts and welds as easy as the standard grades of PP.
  • Impact Strength- 5 times the impact of standard PP; less breakdowns in the field.
  • Extruded Sheet- Offers the best consistency in gauge tolerance and color.

Information provided by Compression Polymers Corp - Vycom

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.990 g/cc0.0358 lb/in³ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 656510 sec.; ASTM D2240
Tensile Strength, Ultimate 24.1 MPa3500 psiASTM D638
Flexural Modulus 0.931 GPa135 ksiASTM D790
Izod Impact, Notched NBNBASTM D256
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0V-0ETL Labs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene, Flame Retardant
A. Schulman POLYFLAM™ RPP 1133 Flame Retardant, Copolymer Polypropylene
A. Schulman POLYFLAM™ RPP 1360 Non-Halogenated Homopolymer Polypropylene
E-Polymers TEKAFIN® PH40FR Flame Retardant Heat Resistance Compounded-PP
Lotte Advanced Materials Infino® HN-1064IA PC, Unreinforced FR

PCPCV03 / 29075

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.