MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chi Mei Polyrex® PG-80 Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Molded, Unreinforced

Material Notes: High strength

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Melt Flow 4.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
4.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
Melt Volume Rate (ml/10 min); ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 144 MPa20900 psiH358/30; ISO 2039-1
Tensile Strength at Break 45.0 MPa6530 psi50 mm/min; ISO 527
Tensile Strength, Yield 47.0 MPa6820 psi50 mm/min; ISO 527
Elongation at Break 5.0 %5.0 %50 mm/min; ISO 527
Flexural Strength 68.0 MPa9860 psi2 mm/min; ISO 178
Flexural Modulus 2.40 GPa348 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO) 2.00 kJ/m²0.952 ft-lb/in²ISO 180/1A
Izod Impact, Unnotched (ISO) 9.00 kJ/m²4.28 ft-lb/in²ISO 180/1C
Charpy Impact Unnotched 1.10 J/cm²5.24 ft-lb/in²ISO 179
Charpy Impact, Notched 0.300 J/cm²1.43 ft-lb/in²ISO 179
Impact 3.03.0Impact Flexural Test Notched (KJ/m²)
 1717Impact Flexural Test Unnotched (KJ/m²)
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °Funannealed; ISO 75
 94.0 °C201 °Fannealed; ISO 75
Vicat Softening Point  94.0 °C
@Load 5.00 kg
201 °F
@Load 11.0 lb
50°C/hr; ISO 306
 96.0 °C
@Load 1.00 kg
205 °F
@Load 2.20 lb
50°C/hr; ISO 306
 97.0 °C
@Load 5.00 kg
207 °F
@Load 11.0 lb
120°C/hr; ISO 306
 102 °C
@Load 1.00 kg
216 °F
@Load 2.20 lb
120°C/hr; ISO 306
Flammability, UL94 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
UL 94

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chi Mei Polyrex® PG-33 Polystyrene
Chi Mei Polyrex® PG-80N Polystyrene
Chi Mei Polyrex® PG-22 Polystyrene
Chi Mei Polyrex® PH-888H Polystyrene - High Impact
Chi Mei Polyrex® PH-55Y Polystyrene - Food

PCHI934 / 109422

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.