MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BorsodChem ONGROSTYR F-IV Expandable Polystyrene (EPS)  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: ONGROSTYR F-IV is an expandable, flame-retardant styrene homopolymer, produced by suspension polymerization. The product meets the requirements of DIN 4102 and of B1 class of building materials, i.e. "low inflammability grade".

Field of application: ONGROSTYR F-IV is suitable for traditional and vacuum molded processing. The minimum apparent density of the end-product is 12 kg/m3, by post-foaming it is 8 kg/m3. This type is recommended for insulation in the building industry and for light blocks with recycled flame retardant EPS and sound absorbing flooring sheets.

Information provided by BorsodChem Rt.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Apparent Bulk Density 0.550 - 0.650 g/cc0.0199 - 0.0235 lb/in³MSZ ISO 60:1994
Particle Size 1700 - 2800 µm1700 - 2800 µmmin 92%; BC HSZ 326:2001/1 screening
Viscosity 1.7 cP1.7 cPUbbelohde viscosity meter
 
Descriptive Properties
Blowing agent content (pentane),%5.5 - 6.5
Residual Monomer Content max %0.2
Water Content, %, max1.4

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical R320 EPS, Flame Retardant
Lotte Advanced Materials Starex® SG-501 Expandable Polystyrene (EPS) High Expansion
BASF Styropor® F 215 L-N Expandable Polystyrene
BASF Peripor® 200 Expandable Polystyrene
IRPC Polimaxx Pentfoam 422F Expandable Polystyrene

PBORS11 / 27535

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.