MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Thermoseal

Klinger Thermoseal RG-S140 PTG Gasketing
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Thermoseal RG-S140 is a controlled-swell gasket material that provides excellent sealing w here initial gasket conformability is required to compensate for flange out of flatness or roughness. After establishing initial sealability, the styrene butadiene binder fully vulcanizes with time and heat of component operation to provide long lasting performance. RG-S140 contains a unique blend of aramid, mineral, and cellulose fibers as well as mineral fillers to provide enhanced crush and temperature resistance. A factory applied release coating on both sides aids in flange removal. Continuous roll lengths allow efficient and economical fabrication with high speed die cutting equipment. Typical applications include gaskets for sealing hot oil or coolant in machinery including small engines and automotive and heavy duty diesel engines with intermittent operating temperatures up to 550° F (288° C)

Information provided by Thermoseal Inc.

Vendors: Thermoseal Inc. is the exclusive North American producer of Klinger Fluid Sealing products, including popular lines: Sealex, Klingersil and Topchem and our new Performance Technology Group of products. Visit us at Thermosealinc.com or call 1-800-990-7325 to speak with a fluid sealing specialist.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ASTM F1315
Thickness 800 microns31.5 milThickness tested
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 6.00 MPa>= 870 psiASTM F152
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 288 °C550 °Fintermittent
 
Descriptive Properties
Binder TypeStyrene Butadiene Rubber (Partially Vulcanized)
Compressibility12-25 percentASTM F36J
Recovery>35 percentASTM F36J
Thickness Increase<60%After immersion in Oil IRM903
Weight Increase<45%After immersion in Oil IRM903

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Klinger Thermoseal ML-N562 PTG Gasketing
Klinger Thermoseal ML-5270 PTG Gasketing
Portland Cement with Treated Silica Fume
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M22 Moldable
Klinger Thermoseal RG-S160 PTG Gasketing

PTHERM928 / 146082

Thermoseal

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.