System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Ineos ABS Lustran® ABS 650 Injection Molding Grade
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Material Notes:
Lustran® ABS 650 has high impact strength, high flow, and is injection molding grade.
Lustran® is now a product of INEOS Styrolution. Information provided by the manufacturer.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.04
g/cc
0.0376
lb/in³
ISO 1183
Linear Mold Shrinkage, Transverse
0.0040
-
0.0060
cm/cm
0.0040
-
0.0060
in/in
ISO 294-4
Melt Flow
22
g/10 min
@Load 10.0 kg,
Temperature 220 °C
22
g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell R
110
110
ISO 2039-2
Tensile Strength at Break
33.0
MPa
4790
psi
50 mm/min; ISO 527-1,-2
Tensile Strength, Yield
44.0
MPa
6380
psi
50 mm/min; ISO 527-1,-2
Elongation at Break
20 %
20 %
50 mm/min; acc. ISO 527-1,-2
Tensile Modulus
2.25
GPa
326
ksi
1 mm/min; ISO 527-1,-2
Flexural Strength
68.0
MPa
9860
psi
2 mm/min; ISO 178
Flexural Modulus
2.20
GPa
319
ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO)
9.00
kJ/m²
@Temperature -30.0 °C
4.28
ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
15.0
kJ/m²
@Temperature -20.0 °C
7.14
ft-lb/in²
@Temperature -4.00 °F
ISO 180-1A
22.0
kJ/m²
@Temperature 23.0 °C
10.5
ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
94.0
°C
201
°F
ISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi)
91.0
°C
196
°F
ISO 75-1,-2
Vicat Softening Point
98.0
°C
@Load 5.10 kg
208
°F
@Load 11.2 lb
120°C/hour; ISO 306
Flammability, UL94
HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Optical Properties
Metric
English
Comments
Gloss
87 %
87 %
Angle 60°; ISO 2813
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Bhansali Engineering Abstron KU-650 ABS Super Heat Resistant
Ineos ABS Lustran® ABS 440 Injection Molding Grade
INEOS Styrolution Absolac® 920 ABS
Ineos ABS Lustran® ABS 640 Injection Molding Grade
Ineos ABS Lustran® ABS 970
PINEA948 / 107219
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.