MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Gravi-Tech™ GRV-UR-110-W Polyurethane, PUR
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes:

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 11.0 g/cc11.0 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 2.62 MPa380 psiType I, 5.1 mm/min; ASTM D638
Elongation at Break 10 %10 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 0.276 GPa40.0 ksiType I, 5.1 mm/min; ASTM D638
Flexural Modulus 0.172 GPa24.9 ksiASTM D790
Izod Impact, Notched 1.60 J/cm
@Thickness 6.35 mm,
Temperature 23.0 °C
3.00 ft-lb/in
@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 204 °C360 - 399 °F
Drying Temperature 65.6 °C150 °F
Dry Time 4.00 hour4.00 hour
 
Descriptive Properties
FeaturesHigh Density
 Non-Toxic
FormsPellets
Generic MaterialPUR, Unspecified
Generic NamePolyurethane, Unspecified (PUR, Unspecified)
Processing MethodInjection Molding
Regional AvailabilityAsia Pacific
UsesIndustrial Applications
 Medical/Healthcare Applications
 Projectiles
 Radiation Shielding
 Sporting Goods
 Weighting & Balancing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultraform® N2640 Z2 POM + PUR
Avient Edgetek® UR2-40CF/000 BLACK Polyurethane, PUR
Avient Gravi-Tech™ GRV-UR-080-W Polyurethane, PUR
Evonik VESTAGON® B 1065 PUR System
A. Schulman DuraGrip™ DGR 6030 NC/BK Thermoplastic Elastomer (TPE)

PH0POL0641 / 145210

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.