MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NeoGraf GRAFOIL® GTH Standard Fluid Sealing Adhesive-Backed Tape, Gasket and Thread Tape
Categories: Carbon; Graphite

Material Notes: GRAFOIL® Grade GTH is a pressure sensitive adhesive-backed tape made with GRAFOIL® Grade GTB flexible graphite. It applications include: threaded joints, forming place gaskets, and large diameter flanges. Construction: GRAFOIL® Grade GTB ? 0.0012" thick acrylic adhesive ? 0.0005" thick polyester ? 0.0012" thick acrylic pressure sensitive adhesive ? 74# silicone treated release paper

Formerly a product of GrafTech.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 1.12 g/cc0.0405 lb/in³Standard; Graphite
Thickness 130 microns5.12 milStandard; Graphite, prior to construction and crinkling
 250 microns9.84 milStandard; Graphite, prior to construction and crinkling
 380 microns15.0 milStandard; Graphite, prior to construction and crinkling

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NeoGraf GRAFOIL® GTA Standard Fluid Sealing Graphite Single Layer Gasketing Material
NeoGraf GRAFOIL® GHC Standard Internal Combustion Laminate
Graphite, Carbon, C
BACT Metal-Dylyn® Diamond-Like Nanocomposite Coating
BACT Dylyn® Diamond-Like Nanocomposite Coating

CGRAF944 / 107348

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.