MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

AISI 1050 Steel, as rolled
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Medium Carbon Steel

Material Notes: The composition listed applies only to structural shapes, plates, strip, and welded tubing. Semifinished products for forging, hot-rolled and cold-finished bars, wire rods, and seamless tubing have a carbon range of 0.48 - 0.55%.

Key Words: UNS G10500, EN43A, carbon steels
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.85 g/cc0.284 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 229229
Hardness, Knoop 252252Converted from Brinell
Hardness, Rockwell B 9696Converted from Brinell
Hardness, Rockwell C 1919Converted from Brinell hardness. Value below normal HRC range, for comparison purposes only.
Hardness, Vickers 241241Converted from Brinell
Tensile Strength, Ultimate 725 MPa105000 psi
Tensile Strength, Yield 415 MPa60200 psi
Elongation at Break 20 %20 %In 50 mm
Reduction of Area 40 %40 %
Modulus of Elasticity 205 GPa29700 ksiTypical for steel
Bulk Modulus 160 GPa23200 ksiTypical for steel
Poissons Ratio 0.290.29Typical For Steel
Shear Modulus 80.0 GPa11600 ksiTypical for steel
Izod Impact 31.0 J22.9 ft-lb
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.0000163 ohm-cm
@Temperature 0.000 °C
0.0000163 ohm-cm
@Temperature 32.0 °F
annealed specimen
 0.0000224 ohm-cm
@Temperature 100 °C
0.0000224 ohm-cm
@Temperature 212 °F
annealed specimen
 0.0000300 ohm-cm
@Temperature 200 °C
0.0000300 ohm-cm
@Temperature 392 °F
annealed specimen
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.486 J/g-°C
@Temperature >=100 °C
0.116 BTU/lb-°F
@Temperature >=212 °F
annealed
Thermal Conductivity 49.8 W/m-K346 BTU-in/hr-ft²-°FTypical steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.47 - 0.55 %0.47 - 0.55 %
Iron, Fe 98.46 - 98.92 %98.46 - 98.92 %As remainder
Manganese, Mn 0.60 - 0.90 %0.60 - 0.90 %
Phosphorus, P <= 0.040 %<= 0.040 %
Sulfur, S <= 0.050 %<= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1050 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1050 Steel, normalized at 900°C (1650°F)
AISI 1050 Steel, annealed at 790°C (1450°F)
AISI 1060 Steel, as rolled
AISI 1050 Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round

M1050E / 7001

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.