MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI Type S15500 (15Cr-5Ni) Precipitation Hardening Stainless Steel, condition H925
Categories: Metal; Ferrous Metal; Stainless Steel; Precipitation Hardening Stainless; T S10000 Series Stainless Steel

Material Notes: Martensitic, precipitative hardening (maraging), combining high strength and hardness with excellent corrosion resistance. Applications include valve parts, fittings and fasteners, shafts, gears, chemical process equipment, paper mill equipment, aircraft components and nuclear reactor components.

Key Words: 15-5 PH, 15-5PH, 15/5 PH, 15/5PH, XM12, AMS 5862, ASME SA705 (XM-12), ASTM A564 (XM-12), ASTM A693 (XM-12), ASTM A705 (XM-12), AFNOR NF A35-581 Z6CNU15.05, DIN 1.4540, DIN X4CrNiCuNb164, Cr-Ni 15-5, UNS S15500, AMS 5658, AMS 5659, AMS 5826
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1317 MPa191000 psi
 400 MPa
@Temperature 650 °C
58000 psi
@Temperature 1200 °F
 758 MPa
@Temperature 540 °C
110000 psi
@Temperature 1000 °F
 1027 MPa
@Temperature 425 °C
149000 psi
@Temperature 797 °F
 1096 MPa
@Temperature 315 °C
159000 psi
@Temperature 599 °F
 1158 MPa
@Temperature 205 °C
168000 psi
@Temperature 401 °F
 1462 MPa
@Temperature -73.0 °C
212000 psi
@Temperature -99.4 °F
Tensile Strength, Yield 1213 MPa175900 psi
 317 MPa
@Strain 0.2 %,
Temperature 650 °C
46000 psi
@Strain 0.2 %,
Temperature 1200 °F
 634 MPa
@Strain 0.2 %,
Temperature 540 °C
92000 psi
@Strain 0.2 %,
Temperature 1000 °F
 965 MPa
@Strain 0.2 %,
Temperature 315 °C
140000 psi
@Strain 0.2 %,
Temperature 599 °F
 1048 MPa
@Strain 0.2 %,
Temperature 205 °C
152000 psi
@Strain 0.2 %,
Temperature 401 °F
 1372 MPa
@Strain 0.2 %,
Temperature -73.0 °C
199000 psi
@Strain 0.2 %,
Temperature -99.4 °F
 1414 MPa
@Strain 0.2 %,
Temperature 425 °C
205100 psi
@Strain 0.2 %,
Temperature 797 °F
Elongation at Break 16 %16 %gage length is 4 times diameter
 14 %
@Temperature 315 °C
14 %
@Temperature 599 °F
gage length is 4 times diameter
 15 %
@Temperature 425 °C
15 %
@Temperature 797 °F
gage length is 4 times diameter
 15 %
@Temperature 205 °C
15 %
@Temperature 401 °F
gage length is 4 times diameter
 17 %
@Temperature -73.0 °C
17 %
@Temperature -99.4 °F
gage length is 4 times diameter
 17 %
@Temperature 540 °C
17 %
@Temperature 1000 °F
gage length is 4 times diameter
 26 %
@Temperature 650 °C
26 %
@Temperature 1200 °F
gage length is 4 times diameter
Charpy Impact 79.0 J58.3 ft-lb
 9.00 J
@Temperature -73.0 °C
6.64 ft-lb
@Temperature -99.4 °F
 22.0 J
@Temperature -40.0 °C
16.2 ft-lb
@Temperature -40.0 °F
 38.0 J
@Temperature -12.0 °C
28.0 ft-lb
@Temperature 10.4 °F
 
Electrical PropertiesMetricEnglishComments
Magnetic Permeability 9595approximate value for the annealed condition at RT
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.070 %<= 0.070 %
Chromium, Cr 14.8 %14.8 %
Copper, Cu 3.5 %3.5 %
Iron, Fe 75 %75 %
Manganese, Mn <= 1.0 %<= 1.0 %
Nb + Ta 0.30 %0.30 %
Nickel, Ni 4.5 %4.5 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type S15500 (15Cr-5Ni) Precipitation Hardening Stainless Steel transverse direction, condition H900
AISI Type S15500 (15Cr-5Ni) Precipitation Hardening Stainless Steel, condition H1025
AISI Type S15500 (15Cr-5Ni) Precipitation Hardening Stainless Steel longitudinal direction, condition H900
AISI Type S15500 (15Cr-5Ni) Precipitation Hardening Stainless Steel longitudinal direction, condition H1025
AISI Type S15500 (15Cr-5Ni) Precipitation Hardening Stainless Steel transverse direction, condition H925

MQM15AH / 13520

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.