MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Geon® Performance Solutions Vinyl Flexible B6D00 Polyvinyl Chloride, Flexible
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes:

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.41 g/cc1.41 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0080 - 0.012 cm/cm0.0080 - 0.012 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 595915 sec; ASTM D2240
 6969ASTM D2240
Tensile Strength at Break 21.4 MPa3100 psiType IV, 510 mm/min; ASTM D638
Tensile Stress at Strain 19.3 MPa
@Strain 100 %
2800 psi
@Strain 100 %
Type IV, 510 mm/min; ASTM D638
Elongation at Break 280 %280 %Type IV, 510 mm/min; ASTM D638
Compression Set 90 %
@Temperature 23.0 °C,
Time 79200 sec
90 %
@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
Clash Berg Modulus 1.10 GPa160 ksiASTM D1043
 0.310 GPa
@Temperature 2.00 °C
45.0 ksi
@Temperature 35.6 °F
ASTM D1043
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -3.33 °C26.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Melt Temperature 179 - 185 °C354 - 365 °F
 193 - 204 °C379 - 399 °F
 
Descriptive Properties
Agency RatingsNSF 51BLACK 2999. Max. Temp. of use = 100 degrees F.
FeaturesMedium Gloss
FormsPellets
Generic MaterialPVC, Flexible
Generic NamePolyvinyl Chloride, Flexible
Processing MethodExtrusion
 Injection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesConstruction Applications
 Fencing & Decking

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Packaging 2188GC Polyvinyl Chloride, Rigid

PH0POL0085 / 144654

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.