MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Atom Adhesives AA-BOND F253 Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: AA-BOND F253 is a low viscosity, high temperature, two-part epoxy formulation that changes color during the curing process to indicate cure status.

Appearance: Unmixed-Light Yellow; Mixed – Greenish Blue; Cured – Reddish Amber

Cure Type: Heat cure or Room Temperature

Benefits:

  • Good impact and thermal shock resistance
  • Demonstrates low stress
  • Yields excellent pot and polish connections
  • It is also resistant to water and weather, vapors and gases.
  • Low viscosity
  • High temperature
Mix Ratio by weight: 100:10/Resin:Hardener

Substrates: Wide variety of fiber optic and optical materials that includes most metals, ceramics, glass and many plastics

Information provided by Atom Adhesives

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccuncured
Solids Content 100 %100 %reactive, uncured
Volatile Organic Compounds (VOC) Content 19.6 g/l19.6 g/l
Water Absorption 0.0040 %0.0040 %
Viscosity 1800 cP1800 cPuncured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8888cured
Shear Strength 18.6 MPa2700 psicured, lap, Alum to Alum
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.3 µm/m-°C11.3 µin/in-°Fcured, Below Tg
 62.4 µm/m-°C34.7 µin/in-°Fcured, Above Tg
Maximum Service Temperature, Air 175 °C347 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Glass Transition Temp, Tg 116 °C241 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.561.56cured
 
Processing PropertiesMetricEnglishComments
Cure Time  1.00 min
@Temperature 150 °C
0.0167 hour
@Temperature 302 °F
 5.00 min
@Temperature 125 °C
0.0833 hour
@Temperature 257 °F
 15.0 min
@Temperature 100 °C
0.250 hour
@Temperature 212 °F
Pot Life 60.0 min60.0 minuncured
 
Descriptive Properties
Thixotropic Index1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Atom Adhesives AA-BOND F112 Epoxy Adhesive
Atom Adhesives AA-DUCT 2979 Epoxy Adhesive
Atom Adhesives AA-DUCT N02 Epoxy Adhesive
Epoxy Technology EPO-TEK® P1011 Electrically Conductive Modified Polyimide
Tra-Con Tra-Bond F253 Color Keyed High Temperature Epoxy Adhesive

PATOM024 / 172339

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.