MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient LubriOne™ NN-30GF/15T Black Polyamide 66 (Nylon 66)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. LubriOne compounds have been demonstrated to reduce friction, noise, vibration, heat buildup and improve product durability.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.49 g/cc1.49 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm0.0020 - 0.0030 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 152 MPa22000 psiType I, 5.1 mm/min; ASTM D638
Elongation at Break 3.0 %3.0 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 8.27 GPa1200 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 228 MPa33100 psiASTM D790
Flexural Modulus 8.27 GPa1200 ksiASTM D790
Izod Impact, Notched 1.10 J/cm
@Thickness 6.35 mm,
Temperature 23.0 °C
2.06 ft-lb/in
@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Coefficient of Friction, Dynamic 0.590.59vs. Metal - Dynamic; ASTM D1894
Coefficient of Friction, Static 0.460.46vs. Steel; ASTM D1894
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 34.0 µm/m-°C18.9 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 254 °C
@Thickness 3.18 mm
489 °F
@Thickness 0.125 in
Annealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Mold Temperature 65.6 - 93.3 °C150 - 200 °F
Drying Temperature 71.1 - 82.2 °C160 - 180 °F
 
Descriptive Properties
AppearanceBlack
FeaturesGood Wear Resistance
 Lubricated
FormsPellets
Generic MaterialNylon 66
Generic NamePolyamide 66 (Nylon 66)
Regional AvailabilityNorth America
RoHS ComplianceRoHS Compliant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Edgetek® NN-30GF/000 Polyamide 66 (Nylon 66)
Avient LubriOne™ ATH-05KV/000 Acetal (POM) Homopolymer
Avient LubriOne™ PC-1000 Polycarbonate
Avient LubriOne™ PS-30GF/15T Natural Polybutylene Terephthalate (PBT)
Envalior Stanyl® TW200F6 PA46-GF30, Conditioned, 30% Glass Filled, Heat Stabilized

PH0POL1010 / 145579

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.