MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips Sumika Marlex® BHD-120 Homopolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Highly Rigid, Talc-Filled Homopolymer.

Applications: Automotive, under-the-hood

Conditioning after Molding: 48 hr at 23°C

Nominal Shrinkage: 0.7-0.9%

    Drying conditions
  • Temperature: 80-100°C
  • Time: 2 hours minimum, 4 hours maximum
  • Device: Desiccant Dryer
  • Moisture content: 0.1 wt% max.

    Molding Temperatures
  • Rear Temperature: 145-200°C
  • Middle Temperature: 210-235°C
  • Front and Nozzle Temps: 210-235°C
  • Stock Temperature: 205-260°C
  • Mold Temperature: 23-50°C

    Processing conditions
  • Suggested shot size: 50-70%
  • First stage injection pressure: Maximize
  • Screw Speed: 30-60%
  • Packing pressure: Minimize
  • Back Pressure: 50-150 psi

Other molding considerations: Melt temperature above 260°C may cause resin degradation and changes to resin properties. To improve dispersion of color concentrates use a screw with a mixing zone or mixing nozzle.

Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. This product had been discontinued prior to the shutdown announcement.

Key Words: Information Provided by Chevron Phillips Chemical
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ASTM D1505
 1.24 g/cc0.0448 lb/in³ISO 1183
Linear Mold Shrinkage 0.0070 - 0.0090 cm/cm0.0070 - 0.0090 in/in
Melt Flow  12 g/10 min
@Temperature 230 °C
12 g/10 min
@Temperature 446 °F
ASTM D1238
 12 g/10 min
@Temperature 230 °C
12 g/10 min
@Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 36.0 MPa5220 psi50 mm/min; ISO 527
 37.0 MPa5370 psi50 mm/min; ASTM D638
Flexural Modulus 4.50 GPa653 ksiSecant, 1.3 mm/min; ASTM D790
 5.33 GPa773 ksi2.0 mm/min; ISO 178
Izod Impact, Notched 0.210 J/cm0.393 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 2.00 kJ/m²0.952 ft-lb/in²ISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 140 °C284 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C189 °FISO 75
 95.0 °C203 °FASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Hostacom™ GP622 Polypropylene Homopolymer
Inno-Comp INNOPOL® CS 1-3120 N DEL 20% Talc Filled Polypropylene Homopolymer
Teknor Apex Sinpolene TPP1020 Polypropylene
Spartech DP5120 Talc Filled Homopolymer
Avient Maxxam™ PPH-20G Nat Polypropylene Homopolymer (PP Homopolymer)

PPPP002 / 90439

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.