MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total MDPE HF 513 Medium Density Polyethylene, Blown Film
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Film Grade

Material Notes: MDPE HF 513 is a medium density polyethylene produced by slurry loop low pressure process with hexene as co-monomer.

MDPE HF 513 is a semi-high molecular weight polyethylene giving excellent mechanical properties. It shows a broad molecular weight distribution ensuring outstanding processability.

MDPE HF 513 can be used alone, blended or coextruded in a wide variety of blown film applications : consumer, industrial, food or hygiene packaging.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.934 g/cc0.934 g/ccISO 1183
Melt Flow  0.15 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.15 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 14.5 g/10 min
@Load 21.60 kg,
Temperature 190 °C
14.5 g/10 min
@Load 47.62 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD  18.0 MPa
@Thickness 0.0400 mm
2610 psi
@Thickness 0.00157 in
ISO 527-3
 20.0 MPa
@Thickness 0.0200 mm
2900 psi
@Thickness 0.000787 in
ISO 527-3
Film Tensile Strength at Yield, TD  18.0 MPa
@Thickness 0.0400 mm
2610 psi
@Thickness 0.00157 in
ISO 527-3
 19.0 MPa
@Thickness 0.0200 mm
2760 psi
@Thickness 0.000787 in
ISO 527-3
Film Elongation at Break, MD  400 %
@Thickness 0.0200 mm
400 %
@Thickness 0.000787 in
ISO 527-3
 540 %
@Thickness 0.0400 mm
540 %
@Thickness 0.00157 in
ISO 527-3
Film Elongation at Break, TD  500 %
@Thickness 0.0200 mm
500 %
@Thickness 0.000787 in
ISO 527-3
 620 %
@Thickness 0.0400 mm
620 %
@Thickness 0.00157 in
ISO 527-3
Flexural Modulus 0.620 GPa
@Strain <=0.25 %
89.9 ksi
@Strain <=0.25 %
ISO 178
Elmendorf Tear Strength, MD  1.10 g/micron
@Thickness 0.0200 mm
27.9 g/mil
@Thickness 0.000787 in
ISO 6383-1
 2.40 g/micron
@Thickness 0.0400 mm
61.0 g/mil
@Thickness 0.00157 in
ISO 6383-1
Elmendorf Tear Strength, TD  13.8 g/micron
@Thickness 0.0200 mm
351 g/mil
@Thickness 0.000787 in
ISO 6383-1
 18.9 g/micron
@Thickness 0.0400 mm
480 g/mil
@Thickness 0.00157 in
ISO 6383-1
Dart Drop Test  220 g
@Thickness 0.0200 mm
0.485 lb
@Thickness 0.000787 in
ISO 7765-1
 290 g
@Thickness 0.0400 mm
0.639 lb
@Thickness 0.00157 in
ISO 7765-1
Film Tensile Strength at Break, MD  55.0 MPa
@Thickness 0.0400 mm
7980 psi
@Thickness 0.00157 in
ISO 527-3
 65.0 MPa
@Thickness 0.0200 mm
9430 psi
@Thickness 0.000787 in
ISO 527-3
Film Tensile Strength at Break, TD  52.0 MPa
@Thickness 0.0200 mm
7540 psi
@Thickness 0.000787 in
ISO 527-3
 52.0 MPa
@Thickness 0.0400 mm
7540 psi
@Thickness 0.00157 in
ISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 125 °C257 °FISO 11357
Vicat Softening Point 118 °C244 °FISO 306
 
Processing PropertiesMetricEnglishComments
Processing Temperature 190 - 220 °C374 - 428 °FExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman POLYBATCH™ Violet 4022 Concentrate Based In Polyethylene
Equate EFDA-7047 LLDPE Film Extrusion Resin
Total MDPE 3802 Blue Medium Density Polyethylene, Stripes
Total MDPE 3802 B Medium Density Polyethylene, Pipes & Fittings
Total MDPE HT 514 Medium Density Polyethylene, Blown Film

PTOTAL756 / 130481

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.