MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Apec® RW1697 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: MVR (330 °C/2.16 kg) 45 cm³/10 min; easy release; low viscosity; softening temperature (VST/B 120) = 157°C

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Moisture Absorption at Equilibrium 0.12 %0.12 %ISO 62
Water Absorption at Saturation 0.30 %0.30 %ISO 62
Linear Mold Shrinkage, Flow 0.0070 cm/cm0.0070 in/in60 x 60 x 2 mm3; 500 bar holding pressure; ISO 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/in60 x 60 x 2 mm3; 500 bar holding pressure; ISO 2577
Melt Flow 45 g/10 min
@Load 2.16 kg,
Temperature 330 °C
45 g/10 min
@Load 4.76 lb,
Temperature 626 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 68.0 MPa9860 psi50 mm/min; ISO 527-1,-2
Elongation at Break 50 %50 %50 mm/min; ISO 527-1,-2
Elongation at Yield 6.0 %6.0 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2.50 GPa363 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 110 MPa16000 psi5 mm/min; ISO 178
Flexural Modulus 2.50 GPa363 ksi2 mm/min; ISO 178
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.900 J/cm²
@Thickness 3.00 mm,
Temperature 23.0 °C
4.28 ft-lb/in²
@Thickness 0.118 in,
Temperature 73.4 °F
acc. ISO 179/1eA
 0.900 J/cm²
@Thickness 3.00 mm,
Temperature -30.0 °C
4.28 ft-lb/in²
@Thickness 0.118 in,
Temperature -22.0 °F
acc. ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F
@Temperature 73.4 - 131 °F
ASTM E831
CTE, linear, Transverse to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F
@Temperature 73.4 - 131 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 149 °C300 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 137 °C279 °FISO 75-1,-2
Vicat Softening Point 157 °C
@Load 5.10 kg
315 °F
@Load 11.2 lb
120°C/h; ISO 306
Flammability, UL94  HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 95 %
@Thickness 3.00 mm
95 %
@Thickness 0.118 in
ISO 5036-1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 330 °C626 °FInjection; ISO 294
Mold Temperature 100 °C212 °FInjection; ISO 294
Injection Velocity 200 mm/sec7.87 in/secISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röhm PLEXIGLAS® XT Clear 0A070 UV transmitting PMMA
Zeon Specialty Materials ZEONEX® 790R Cyclo Olefin Polymer
Covestro Apec® 1600 Polycarbonate
Covestro Apec® 1605 Polycarbonate
Covestro Makrolon® AU sheet Polycarbonate

PCOVEST0011 / 201794

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.