MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Silver, Ag
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Pure Element

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 10.491 g/cc0.37901 lb/in³
 9.00 g/cc
@Temperature 1300 °C
0.325 lb/in³
@Temperature 2370 °F
Liquid
 9.10 g/cc
@Temperature 1195 °C
0.329 lb/in³
@Temperature 2183 °F
Liquid
 9.20 g/cc
@Temperature 1092 °C
0.332 lb/in³
@Temperature 1998 °F
Liquid
 9.26 g/cc
@Temperature 1000 °C
0.335 lb/in³
@Temperature 1830 °F
Liquid
 9.30 g/cc
@Temperature 960.5 °C
0.336 lb/in³
@Temperature 1761 °F
Liquid
Vapor Pressure  1.013 bar
@Temperature 1304 °C
759.8 torr
@Temperature 2379 °F
 10.13 bar
@Temperature 1510 °C
7598 torr
@Temperature 2750 °F
 101.3 bar
@Temperature 1783 °C
75980 torr
@Temperature 3241 °F
 1013 bar
@Temperature 2163 °C
759800 torr
@Temperature 3925 °F
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 107.8682107.86821995
Atomic Number 4747
Thermal Neutron Cross Section 63 barns/atom63 barns/atom
X-ray Absorption Edge 0.4858 Å0.4858 ÅK
 3.23824 Å3.23824 ÅLI
 3.49478 Å3.49478 ÅLII
 3.67288 Å3.67288 ÅLIII
Electrode Potential 0.799 V0.799 V
Electronegativity 1.931.93Pauling
Ionic Radius 0.89 Å0.89 ÅCrystal Ionic Radius for Valence +2
 1.26 Å1.26 ÅCrystal Ionic Radius for Valence +1
Electrochemical Equivalent 4.025 g/A/h4.025 g/A/h
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 2525Annealed
Tensile Strength, Ultimate 140 MPa20300 psiAnnealed
Modulus of Elasticity 76.0 GPa11000 ksi
Poissons Ratio 0.370.37Annealed
 0.390.39Hard drawn
Shear Modulus 27.8 GPa4030 ksiCalculated; Annealed
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000155 ohm-cm0.00000155 ohm-cm
Magnetic Susceptibility 2.0e-72.0e-7cgs/g
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 105 J/g45.2 BTU/lb
Heat of Vaporization 2332 J/g1003 BTU/lb
CTE, linear  19.6 µm/m-°C
@Temperature 20.0 - 100 °C
10.9 µin/in-°F
@Temperature 68.0 - 212 °F
 19.9 µm/m-°C
@Temperature 0.000 - 250 °C
11.1 µin/in-°F
@Temperature 32.0 - 482 °F
 20.6 µm/m-°C
@Temperature 0.000 - 500 °C
11.4 µin/in-°F
@Temperature 32.0 - 932 °F
 22.4 µm/m-°C
@Temperature 0.000 - 900 °C
12.4 µin/in-°F
@Temperature 32.0 - 1650 °F
Specific Heat Capacity 0.234 J/g-°C0.0559 BTU/lb-°F
Thermal Conductivity 419 W/m-K2910 BTU-in/hr-ft²-°F
Melting Point 961.93 °C1763.5 °F
Boiling Point 2162 °C3924 °F
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.055
@Temperature 700 °C
0.055
@Temperature 1290 °F
Reflection Coefficient, Visible (0-1) 0.900.90
 
Component Elements PropertiesMetricEnglishComments
Silver, Ag 100 %100 %
 
Descriptive Properties
CAS Number7440-22-4

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum, Al
Gold, Au
Copper, Cu; Annealed
Americium, Am
Iron, Fe

AMEAg00 / 2

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.