MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Refractory Metals

Mo-44.5 Re Molybdenum Rhenium Alloy, Annealed
Categories: Metal; Nonferrous Metal; Molybdenum Alloy; Refractory Metal

Material Notes: Annealed applies only to tensile; other property values are typical of this alloy. Ductile to brittle transition temperature (DBBT) (-273) - (-173) °C. Stress relieving temperature 1000-1200°C. Recrystallization Temperature 1300-1550°C. Bcc crystal lattice.

Key Words: Rhenium Molybdenum Alloys
Vendors: Elmet Technologies is a 100% US owned and operated, fully integrated manufacturer of Molybdenum, Tungsten and related alloys such as TZM, WHA & MoLa. At our 220,000 sqr/ft plant in Lewiston, Maine, Elmet manufactures W & Mo pure powders plus rod, wire, plate, sheet & foil in additional to offering fabrication and machining services. ITAR, ISO and AS9100 registered. www.elmettechnologies.com

PLANSEE SE: Whether it's high temperatures, aggressive chemicals or extreme mechanical loading: PLANSEE supplies a suitable product solution in refractory metals or composite materials. As the world market leader in powder metallurgically produced high performance materials we combine outstanding materials knowledge with profound applications and technology know-how. Visit us at www.plansee.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 13.5 g/cc0.488 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 990 MPa144000 psi
 220 MPa
@Temperature 1200 °C
31900 psi
@Temperature 2190 °F
 590 MPa
@Temperature 800 °C
85600 psi
@Temperature 1470 °F
Tensile Strength, Yield 780 MPa113000 psi
 170 MPa
@Temperature 1200 °C
24700 psi
@Temperature 2190 °F
 370 MPa
@Temperature 800 °C
53700 psi
@Temperature 1470 °F
Modulus of Elasticity 365 GPa52900 ksi
Poissons Ratio 0.2850.285
Shear Modulus 132 GPa19100 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000220 ohm-cm0.0000220 ohm-cmTemp Coefficient is 0.0017/°C 20-1000°C.
Critical Superconducting Temperature 10.9 K10.9 K
 
Thermal PropertiesMetricEnglishComments
CTE, linear  5.72 µm/m-°C
@Temperature 500 °C
3.18 µin/in-°F
@Temperature 932 °F
 6.45 µm/m-°C
@Temperature 1000 °C
3.58 µin/in-°F
@Temperature 1830 °F
Thermal Conductivity 36.8 W/m-K255 BTU-in/hr-ft²-°F
Melting Point 2450 °C4440 °F
Maximum Service Temperature, Air 725 °C1340 °Fsharp increase in oxidation
 
Component Elements PropertiesMetricEnglishComments
Molybdenum, Mo 55.5 %55.5 %
Rhenium, Re 44.5 %44.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mo-47.5 Re Molybdenum Rhenium Alloy, Annealed
Plansee MoRe41 Molybdenum-Rhenium
Mo-47.5 Re Molybdenum Rhenium Alloy, Deformed
Mo-30Re Molybdenum Rhenium Alloy, Stress Relief Annealed
Plansee MoRe5 Molybdenum-Rhenium

MRMo30 / 13895

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.