MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Petrothene® NA870252 Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: Applications
PETROTHENE NA 870-252 exhibits an excellent balance of toughness and softness, with excellent dimensional stability. Typical applications include caps and closures, housewares, toys, containers and novelty items.

Regulatory Status
NA 870-252 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply.

Processing Techniques
Specific recommendations for processing NA 870-252 can only be made when the processing conditions, equipment and end use are known.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.922 g/cc0.0333 lb/in³ASTM D1505
Melt Flow 38 g/10 min38 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4141ASTM D2280
Tensile Strength at Break 8.96 MPa1300 psiCrosshead Speed - 20 in/min; ASTM D638
Tensile Strength, Yield 12.8 MPa1850 psiCrosshead Speed - 20 in/min; ASTM D638
Elongation at Yield 13 %13 %ASTM D638
Flexural Modulus, 1% Secant 228 MPa33000 psiCrosshead Speed - 1/2 in/min; ASTM D790
2% Secant Modulus 0.186 GPa27.0 ksiCrosshead Speed - 1/2 in/min; ASTM D790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 86.0 °C187 °FASTM D1525
Brittleness Temperature -25.0 °C-13.0 °FF50, Test method has been found useful for specification purposes, but does not necessarily indicate the lowest temperature at which the material may be used.; ASTM D746
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake EM184AA Low Density Polyethylene
M. Holland Company MTEGRITY™ LD700 LDPE
Dow LDPE 955I Low Density Polyethylene
LyondellBasell Petrothene® NA217000 Low Density Polyethylene
Celanese AT 418 Low Density Polyethylene (LDPE)

PEQU0547 / 37017

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.