MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LATI Latamid 66 H2 G/35-V0KB PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled; Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.46 g/cc0.0527 lb/in³
Linear Mold Shrinkage, Flow 0.0035 - 0.0060 cm/cm0.0035 - 0.0060 in/in
Linear Mold Shrinkage, Transverse 0.0075 - 0.0105 cm/cm0.0075 - 0.0105 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  80.0 MPa
@Temperature 150 °C
11600 psi
@Temperature 302 °F
 90.0 MPa
@Temperature 120 °C
13100 psi
@Temperature 248 °F
 110 MPa
@Temperature 90.0 °C
16000 psi
@Temperature 194 °F
 145 MPa
@Temperature 60.0 °C
21000 psi
@Temperature 140 °F
 185 MPa
@Temperature 23.0 °C
26800 psi
@Temperature 73.4 °F
Elongation at Break  2.3 %
@Temperature 23.0 °C
2.3 %
@Temperature 73.4 °F
 2.9 %
@Temperature 60.0 °C
2.9 %
@Temperature 140 °F
 3.8 %
@Temperature 90.0 °C
3.8 %
@Temperature 194 °F
 4.2 %
@Temperature 120 °C
4.2 %
@Temperature 248 °F
 4.5 %
@Temperature 150 °C
4.5 %
@Temperature 302 °F
Tensile Modulus  5.80 GPa
@Temperature 150 °C
841 ksi
@Temperature 302 °F
 6.80 GPa
@Temperature 120 °C
986 ksi
@Temperature 248 °F
 7.70 GPa
@Temperature 90.0 °C
1120 ksi
@Temperature 194 °F
 11.0 GPa
@Temperature 60.0 °C
1600 ksi
@Temperature 140 °F
 12.5 GPa
@Temperature 23.0 °C
1810 ksi
@Temperature 73.4 °F
Charpy Impact Unnotched 8.00 J/cm²38.1 ft-lb/in²
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 450 V450 VA solution
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 130 °C266 °F
Deflection Temperature at 0.46 MPa (66 psi) 260 °C500 °F
Deflection Temperature at 1.8 MPa (264 psi) 255 °C491 °F
Vicat Softening Point 250 °C
@Load 5.00 kg
482 °F
@Load 11.0 lb
Flammability, UL94  V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
Oxygen Index 28 %28 %
Glow Wire Test  960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
GWFI/GWT
 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
GWFI/GWT
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 - 290 °C518 - 554 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 90.0 - 100 °C
@Time 10800 sec
194 - 212 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Niche Polymer POLIXL™ PA66GF35BK PA66, 35% Fiberglass Reinforced, Conditioned
LATI Latiohm 66-08 PD02 G/35 PA66, 35% Glass Fiber Reinforced
Akro-Plastic Akromid® A3 GF 35 1 natural PA 6.6 Dry, 35% Glass Filled, Heat Stabilized

PLATH9717 / 177413

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.