MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman Tenite 350A4861313 Cellulose Acetate Propionate, Clear, Trsp
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Cellulosic; Cellulose Acetate Propionate, Molded

Material Notes: Applications:
  • Blood Therapy
  • Drug Delivery
  • IV Components
  • Medical Devices
  • Surgical Instruments

Product Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenitecellulosic plastics differ with plasticizer levels. Lower plasticizer content yields a harder surface, higher heat resistance, greater rigidity, higher tensile strength, and better dimensional stability. Higher plasticizer content increases impact strength. Tenite cellulosic plastics are available in natural, clear, selected ambers or smoke transparents and black translucent. Color concentrates are available in let-down ratios from 10:1 to 40:1. Tenite Cellulose Acetate Propionate 350-13 has a plasticizer level of 13%. It meets FDA requirements for certain food-contact applications when supplied in specific FDA color numbers.

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Water Absorption 1.5 %
@Time 86400 sec
1.5 %
@Time 24.0 hour
Immersion; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm0.0020 - 0.0060 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8585ASTM D785
Tensile Strength at Break 38.3 MPa5550 psiASTM D638
Tensile Strength, Yield 34.5 MPa5000 psiASTM D638
Elongation at Break 40 %40 %ASTM D638
Flexural Strength 44.9 MPa6510 psiASTM D790
Flexural Modulus 1.586 GPa230.0 ksiASTM D790
Izod Impact, Notched  1.02 J/cm
@Temperature -40.0 °C
1.91 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 3.21 J/cm
@Temperature 23.0 °C
6.01 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 - 1.00e+15 ohm-cm1.00e+13 - 1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.3 - 3.8
@Frequency 1e+6 Hz
3.3 - 3.8
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 11.8 - 18.7 kV/mm300 - 475 kV/inASTM D149
Dissipation Factor 0.010 - 0.15
@Frequency 1e+6 Hz
0.010 - 0.15
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 110 - 170 µm/m-°C61.1 - 94.4 µin/in-°FASTM D696
Specific Heat Capacity 1.26 - 1.67 J/g-°C0.301 - 0.399 BTU/lb-°FDSC
Thermal Conductivity 0.170 - 0.330 W/m-K1.18 - 2.29 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 86.0 °C187 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C172 °FASTM D648
Vicat Softening Point 103 °C217 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.46 - 1.49
@Wavelength 589.3 nm
1.46 - 1.49
@Wavelength 589.3 nm
nD; ASTM D542
Haze <= 8.5 %<= 8.5 %ASTM D1003
Transmission, Visible >= 90 %>= 90 %ASTM E308
 
Descriptive Properties
Formula Number350
Plasticizer13 percent
Soluble Matter Loss0.1 percentASTM D570
Weight Loss on Heating0.6 percentASTM D707, 72 hrs, 80°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Tenite 360A4861307 Cellulose Acetate Propionate, Clear, Trsp
Eastman Tenite 360E4861314 Cellulose Acetate Propionate, Clear, Trsp
Eastman Tenite 105E3V36327 Acetate Clear, Trsp
Eastman Tenite 360E0096914 Cellulose Acetate Propionate, Natural, Trsp
Eastman Tenite 360E4861316 Cellulose Acetate Propionate, Clear, Trsp

PE8832 / 129677

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.