MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Zircar Zirconia ZYZ-3 Zirconia Boards and Discs Insulation
Categories: Ceramic; Machinable Ceramic; Oxide; Zirconium Oxide

Material Notes: Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the low thermal conductivity of zirconia fibers combined with the strength and machinability of a silica bonded material. ZYZ is evenly bonded, allowing it to be machined to tight tolerances and intricate shapes. ZYZ has a lower coefficient of thermal expansion than our Type ZYFB materials.

Type ZYZ is ideally suited for thermal insulation and protection applications under conditions of ultra-high temperatures and in a variety of severe environments. ZYZ is fired at a high temperature to impart good dimensional stability up to 1650°C. ZYZ has good hot strength up to 1400°C and can be used as a self supporting setter for loads equal to twice its own weight up to this temperature. ZYZ produces no smoke or odor and undergoes no physically disruptive phase transitions when heated. ZYZ is available in two forms. ZYZ-3 has a bulk density of 30 pcf and possesses extremely low thermal conductivity. ZYZ-6 has a bulk density of 60 pcf and is stronger than ZYZ-3.

Zirconia loses a small amount of oxygen at very high temperatures in vacuum and inert or reducing atmospheres. Although this reaction results in a color change from white to gray, other properties remain essentially unchanged and insulation effectiveness is not impaired.

Features:

  • Rigid and Machinable
  • Silica Bond for Thermal Shock Resistance
  • Available in Two Densities; 30 & 60 pcf
  • Extreme High Temperature Stability
  • Fibers Stabilized with ~10 wt% Yttria
  • Low Thermal Conductivity
  • Can be Cemented with Zircar Zirconia Cement Type ZR-CE
  • Can be Surface Hardened with Zircar Zirconia Rigidizer Type ZR-RIG
  • Pre-fired and Organic Free

Information provided by Zircar Zirconia.

Key Words: ZrO2, zirconium oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.480 g/cc0.0173 lb/in³
Porosity 91 %91 %
Outgassing - Total Mass Loss 0.00 %0.00 %In vacuum
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 0.280 MPa40.6 psiParallel to thickness
Compressive Yield Strength 0.390 MPa56.6 psiParallel to thickness @ 10% compression
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.00 µm/m-°C
@Temperature 20.0 - 1250 °C
5.00 µin/in-°F
@Temperature 68.0 - 2280 °F
Thermal Conductivity  0.0800 W/m-K
@Temperature 400 °C
0.555 BTU-in/hr-ft²-°F
@Temperature 752 °F
 0.110 W/m-K
@Temperature 800 °C
0.763 BTU-in/hr-ft²-°F
@Temperature 1470 °F
 0.140 W/m-K
@Temperature 1100 °C
0.972 BTU-in/hr-ft²-°F
@Temperature 2010 °F
 0.190 W/m-K
@Temperature 1400 °C
1.32 BTU-in/hr-ft²-°F
@Temperature 2550 °F
 0.230 W/m-K
@Temperature 1650 °C
1.60 BTU-in/hr-ft²-°F
@Temperature 3000 °F
Melting Point 2200 °C3990 °F
Maximum Service Temperature, Air 1650 °C3000 °FContinuous
 1700 °C3090 °FIntermittent
Softening Point 1250 °C2280 °FDilatometric @ 10psi
Shrinkage  1.7 %
@Temperature 1650 °C,
Time 3600 sec
1.7 %
@Temperature 3000 °F,
Time 1.00 hour
perpendicular to thickness
 2.3 %
@Temperature 1650 °C,
Time 86400 sec
2.3 %
@Temperature 3000 °F,
Time 24.0 hour
perpendicular to thickness
 
Component Elements PropertiesMetricEnglishComments
HfO2 1.0 - 2.0 %1.0 - 2.0 %
Y2O3 10 %10 %
ZrO2 83 - 84 %83 - 84 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zircar Zirconia ZYFB-3 Zirconia Boards, Discs, and Cylinders Insulation
Zircar Zirconia ZYF-100 Zirconia Felt Insulation
Zircar Zirconia ZYC Zirconia Cylinders Insulation
Zirconium Oxide, Zirconia, ZrO2
MarkeTech Repton 838 Zirconia + 3 mol% Yttria (YSZ)

C6ZIR003 / 2759

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.