MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 399 X 115069 D Polycarbonate (PC), Carbon Nanotube - Electrically Conductive - ESD Protection
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Conductive

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.23 g/cc1.23 g/ccASTM D 792
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
@Thickness 3.17 mm
0.0060 - 0.0080 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 53.8 MPa7800 psiASTM D 638
Elongation at Break >= 8.0 %>= 8.0 %ASTM D 638
Tensile Modulus 2.07 GPa300 ksiASTM D 638
Flexural Strength 89.6 MPa13000 psiASTM D 790
Flexural Modulus 2.41 GPa350 ksiASTM D 790
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 10 - 1000 ohm-cm10 - 1000 ohm-cmASTM D 257
Surface Resistance 10000 - 1.00e+6 ohm10000 - 1.00e+6 ohmESD STM11.11
Surface Resistivity per Square 1e+05 - 1.00e+7 ohm1e+05 - 1.00e+7 ohmASTM D 257
Static Decay <= 2.0 sec<= 2.0 secMIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 288 - 316 °C550 - 600 °F
Mold Temperature 82.2 - 121 °C180 - 250 °F
Drying Temperature 121 °C250 °F
Dry Time 4 hour4 hour
Moisture Content 0.020 %0.020 %
Dew Point -28.9 °C-20.0 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 382 HEC FR  Polycarbonate (PC) Nickel-Coated Carbon Fiber 15% - Flame Retardant - EMI/ESD
RTP Company RTP 2583 C HEC  Polycarbonate/ABS Alloy (PC/ABS) Nickel-Coated Carbon Fiber 20% - EMI/ESD
RTP Company RTP 1099 X 87257 B Polybutylene Terephthalate (PBT) Carbon Nanotube - ESD Protection - Static Dissipative

PQZWA9171 / 92471

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.