MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

American Beech Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Hardwood. Least easy to work with hand tools. Very good steam bending, fair shaping. Data is based on small, clear, air-dried samples unless specified.

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Fagus grandifolia; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.560 g/cc0.0202 lb/in³Oven Dry Weight/Unseasoned Volume
 0.865 g/cc0.0312 lb/in³Unseasoned*
Cell Length 1.20 mm0.0472 inMature Wood
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 3600 N809 lb (f)Side. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 4200 N944 lb (f)End. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 5800 N1300 lb (f)Side
Tensile Strength, Ultimate 5.24 MPa760 psiPerpendicular to Grain*
 7.00 MPa1020 psiPerpendicular to Grain
Modulus of Rupture 0.0565 GPa8.20 ksiStatic Bending*
 0.103 GPa14.9 ksiIn Bending
Flexural Yield Strength 31.0 MPa4500 psiFiber Stress at Elastic Limit; Static Bending*
 60.0 MPa8700 psiBending stress at proportional limit
Flexural Modulus 8.55 GPa1240 ksiStatic Bending*
 11.7 - 11.9 GPa1700 - 1730 ksiIn Bending
Compressive Strength 4.21 MPa610 psiPerpendicular to Grain*
 7.00 MPa1020 psiPerpendicular to Grain
 17.6 MPa2550 psiParallel to Grain*
 22.6 MPa3280 psiMax Crushing Strength Parallel to Grain*
 50.0 - 50.3 MPa7250 - 7300 psiParallel to Grain
Shear Strength 8.34 MPa1210 psiParallel to Grain*
 13.9 MPa2020 psiOrientation Unknown
Impact 4.24.2in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 1040010400psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 0.00683 J/cm³0.990 in-lb/in³Static Bending*
Work to Maximum Load 0.0862 J/cm³12.5 in-lb/in³Static Bending*
Cleavage 59.0 kN/m337 lb/inRadial surface of failure, Unseasoned*
 92.0 kN/m525 lb/inTangential surface of failure, Unseasoned*
 
Thermal PropertiesMetricEnglishComments
CTE, linear  5.40 µm/m-°C
@Temperature 20.0 °C
3.00 µin/in-°F
@Temperature 68.0 °F
Axial. Typical value for Beech.
 22.0 µm/m-°C
@Temperature 20.0 °C
12.2 µin/in-°F
@Temperature 68.0 °F
Radial; Typical value for Beech.
 34.8 µm/m-°C
@Temperature 20.0 °C
19.3 µin/in-°F
@Temperature 68.0 °F
Tangential. Typical value for Beech.
Specific Heat Capacity 0.390 J/g-°C0.0932 BTU/lb-°FWhite Oak
Thermal Conductivity 0.144 W/m-K1.00 BTU-in/hr-ft²-°FOven Dry
 0.173 W/m-K1.20 BTU-in/hr-ft²-°FWhite Oak
 0.187 W/m-K1.30 BTU-in/hr-ft²-°F12% Moisture Content
Shrinkage 5.1 %5.1 %Radial; Green to Zero Moisture
 11 %11 %Tangential; Green to Zero Moisture
 16.3 %16.3 %Volumetric; Green to Zero Moisture

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
European Beech Wood
American Yellow Birch Wood
American Maple, Rock (Sugar Maple)
American White Oak Wood
American Ash Wood

PTSAO / 71298

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.