MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röchling Glastic 1125 Corrosion-Resistant Panels
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Polyester, TS

Material Notes: Glastic® Corrosion-Resistant Panels are ideal for applications where resistance to both flame, and the splash or spill of laboratory chemicals is important. Glastic® Grade 1125 is asbestos-free, fiberglass-reinforced polyester resin sheet that offers low smoke generation when exposed to flame. This material has very low water absorption characteristics, along with excellent splash and spill resistance to acids, weak bases and aliphatic hydrocarbons. Grade 1125 is UL classified, has high strength, and has a bright white finish(no painting necessary). Some applications include fume hood liners, chemical storage cabinets and wall surfaces.

Information provided by Glastic Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.81 g/cc1.81 g/ccASTM D-792
Water Absorption 0.40 %0.40 %% by wt.; ASTM D-570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 51.7 MPa7500 psiASTM D-638
Tensile Modulus 11.7 GPa1700 ksiASTM D-638
Flexural Strength 145 MPa21000 psiASTM D-790
 88.9 MPa
@Temperature 130 °C
12900 psi
@Temperature 266 °F
ASTM D-790
Compressive Strength 224 MPa32500 psiASTM D-695
Izod Impact, Notched 4.48 J/cm8.40 ft-lb/inASTM D-256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 µm/m-°C
@Temperature 20.0 °C
11.1 µin/in-°F
@Temperature 68.0 °F
ASTM D-696
Thermal Conductivity 0.270 W/m-K1.87 BTU-in/hr-ft²-°FASTM C-177
Flame Spread Index 2020Canadian Calculation; ASTM E-84
 2525United States Calculation; ASTM E-84
Oxygen Index 35 %35 %ASTM D-2863
 
Descriptive Properties
Smoke Developed115ASTM E-84
Standard ColorWhite
UL Recognition File NumberR9599NEMA LI-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RheTech Products P251-01 Polypropylene Copolymer, Black
Röchling Glastic 1120 Corrosion-Resistant Panels
A. Schulman Premi-Glas® 2206-15 CR-SX Fiberglass Reinforced Thermoset SMC
Menzolit Menzolit® SMC 0180 Unsaturated Polyester UP
Overview of materials for High Density Polyethylene (HDPE), Injection Molded

PGLASX0 / 41944

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.